Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 6100 ohm-cm | 6100 ohm-cm | |
BASF Heligoen® Blue K 6850 Color Additive Chemical Structure: Cu-Phthalocyanine alpha instab.Application: Colourant for plastics; PVC-p, PVC-u and UPRecommendations for food applications: BgVV, FDA, FrancePhysical form: PowderInformation pr.. |