Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 5000 ohm-cm | 5000 ohm-cm | |
Nabaltec APYRAL® 200 SM Al(OH)3 APYRAL ® from Nabaltec is an environmentally friendly halogen free product which is used as a flame retardant filler in a wide variety of rubber and polymeric materials. During thermal decompositio.. |
|||
Electrical Resistivity | <= 5000 ohm-cm | <= 5000 ohm-cm | |
Magyar Aluminum ALOLT 90F Aluminum Hydroxide Fine Precipitated Type |
|||
Electrical Resistivity | 5000 ohm-cm | 5000 ohm-cm | |
Shakespeare Resistat® F9422 T040 Nylon 6 Monofilament Resistat F9422, MERGE T040 is composed of forty filaments of conductive nylon 6 yarn. This yarn is twisted and heatset. Each filament has electrically conductive carbon suffused into the surface. .. |
|||
Electrical Resistivity | 5000 ohm-cm | 5000 ohm-cm | |
Shakespeare Resistat® F9416 M040 Nylon 66 Monofilament Resistat F9416, MERGE M040 is composed of forty filaments of conductive nylon 6,6 yarn. This yarn is twisted and heatset. Each filament has electrically conductive carbon suffused into the surface.. |
|||
Electrical Resistivity | >= 5000 ohm-cm | >= 5000 ohm-cm | |
BASF Heligoen® Blue 6989 F Color Additive Description: Extremely reddish, e-phthalocyanine blue with high chroma and excellent flocculation resistanceChemical Structure: Cu-phthalocyanine, alpha-stabPhysical form: PowderSuitable for: Baking.. |
|||
Electrical Resistivity | 5000 ohm-cm | 5000 ohm-cm | |
BASF Heligoen® Blue K 6911 D Color Additive Chemical Structure: Cu-phthalocyanine alpha stabApplication: Colourant for plastics; PVC-p, PVC-u, PUR, LD-PE, HD-PE, PP, PS, SB, SAN, PMMA, PA, PETP, CA/CAB, and UPRecommendations for food applicat.. |
|||
Electrical Resistivity | 5000 ohm-cm | 5000 ohm-cm | |
BASF Heligoen® Blue K 7090 Color Additive Chemical Structure: Cu-phthalocyanine betaApplication: Colourant for plastics; PVC-p, PVC-u, PUR, LD-PE, HD-PE, PP, PS, SB, SAN, PMMA, PA, PETP, CA/CAB, and UPRecommendations for food applications: .. |
|||
Electrical Resistivity | >= 5000 ohm-cm | >= 5000 ohm-cm | |
BASF Heligoen® Blue L 6875 H Color Additive Description: Reddish a-phthalocyanine blue with excellent flocculation resistance and dispersibility.Chemical Structure: Cu-phthalocyanine, alpha-stabPhysical form: PowderSuitable for: Baking system.. |
|||
Electrical Resistivity | >= 5000 ohm-cm | >= 5000 ohm-cm | |
BASF Heligoen® Blue L 6920 Color Additive Chemical Structure: Cu-phthalocyanine, Alpha StablePhysical form: PowderApplication: Pigment for PaintsInformation provided by BASF |
|||
Electrical Resistivity | >= 5000 ohm-cm | >= 5000 ohm-cm | |
BASF Heligoen® Blue L 6990 F Color Additive Description: Highly transparent Phthalocyanine blue pigment with neutral flopChemical Structure: Cu-phthalocyanine, alpha-stabPhysical form: PowderSuitable for: Baking systems, Waterborn systems, Ac.. |
|||
Electrical Resistivity | >= 5000 ohm-cm | >= 5000 ohm-cm | |
BASF Heligoen® Blue L 7072 D Color Additive Description: ß-phthalocyanine blue with excellent dispersibilityChemical Structure: Cu-phthalocyanine, betaPhysical form: PowderSuitable for: Baking systems, Waterborn systems, Acrylic-isocyanate s.. |
|||
Electrical Resistivity | >= 5000 ohm-cm | >= 5000 ohm-cm | |
BASF Heligoen® Blue L 7080 Color Additive Description: ß-phthalocyanine blue for economic formulationsChemical Structure: Cu-phthalocyanine, betaPhysical form: PowderSuitable for: Baking systems, Waterborn systems, Acrylic-isocyanate syste.. |
|||
Electrical Resistivity | 5000 ohm-cm | 5000 ohm-cm | |
BASF Heligoen® Green K 8683 Color Additive Chemical Structure: Cu-phthalocyanine chlorinate Application: Colourant for plastics; PVC-p, PVC-u, PUR, LD-PE, HD-PE, PP, PS, SB, SAN, PMMA, CA/CAB, and UPRecommendations for food applications: BgV.. |
|||
Electrical Resistivity | >= 5000 ohm-cm | >= 5000 ohm-cm | |
BASF Heligoen® Green L 8690 Color Additive Description: Phthalocyanine green with excellent rheologyChemical Structure: Cu-phthalocyanine, chlorinatePhysical form: PowderSuitable for: Baking systems, Waterborn systems, Acrylic-isocyanate sys.. |
|||
Electrical Resistivity | >= 5000 ohm-cm | >= 5000 ohm-cm | |
BASF Paliotol™ Yellow L 2140 Color Additive Description: Isoindoline yellow with high opacity and reddish shade for OEM and industrial coatings.Suitable for: Baking systems, Waterborn systems, Acrylic-isocyanate systems, Acid curing system, A.. |
|||
Electrical Resistivity | >= 5000 ohm-cm | >= 5000 ohm-cm | |
BASF Heligoen® Blue L 6700 F Color Additive Chemical Structure: Cu-phthalocyanine, Epsilon Application: Pigment for PaintsPhysical form: PowderInformation provided by BASF |
|||
Electrical Resistivity | >= 5000 ohm-cm | >= 5000 ohm-cm | |
BASF Heligoen® Blue L 6905 F Color Additive Description: Very brilliant a-phthalocyanine blues with high color strength and excellent flocculation resistance (L 6905 F is more brilliant and stronger than L 6901F).Chemical Structure: Cu-phthal.. |
|||
Electrical Resistivity | 5000 ohm-cm | 5000 ohm-cm | |
BASF Heligoen® Green K 9360 Color Additive Chemical Structure: Cu-phthalocyanine halogenisedApplication: Colourant for plastics; PVC-p, PVC-u, PUR, LD-PE, HD-PE, PP, PS, SB, SAN, PMMA, PETP, CA/CAB, and UPRecommendations for food application.. |
|||
Electrical Resistivity | >= 5000 ohm-cm | >= 5000 ohm-cm | |
BASF Heligoen® Green L 8605 Color Additive Description: Bluish phthalocyanine greenChemical Structure: Cu-phthalocyanine, chlorinatePhysical form: PowderSuitable for: Baking systems, Waterborn systems, Acrylic-isocyanate systems, Acid curing.. |
|||
Electrical Resistivity | >= 5000 ohm-cm | >= 5000 ohm-cm | |
BASF Paliogen® Blue L 6470 Color Additive Description: Transparent Indanthrone blue for effect and solid shades with high fastness propertiesPhysical form: PowderSuitable for: Baking systems, Waterborn systems, Acrylic-isocyanate systems, A.. |
|||
Electrical Resistivity | >= 5000 ohm-cm | >= 5000 ohm-cm | |
BASF Paliogen® Pink L 4790 Color Additive Description: Red pigment with very good weather fastnessSuitable for: Baking systems, Waterborn systems, Acrylic-isocyanate systems, and Airdrying systems.Information provided by BASF |
|||
Electrical Resistivity | >= 5000 ohm-cm | >= 5000 ohm-cm | |
BASF Paliogen® Red L 3880 HD Color Additive Description: Perylene reds for shades with high brilliancy and opacitySuitable for: Baking systems, Waterborn systems, Acrylic-isocyanate systems, Acid curing systems, Amine curing systems and Aird.. |
|||
Electrical Resistivity | >= 5000 ohm-cm | >= 5000 ohm-cm | |
BASF Paliogen® Red L 3910 HD Color Additive Description: Perylene reds for shades with high brilliancy and opacitySuitable for: Baking systems, Waterborn systems, Acrylic-isocyanate systems, Acid curing systems, Amine curing systems and Aird.. |
|||
Electrical Resistivity | >= 5000 ohm-cm | >= 5000 ohm-cm | |
BASF Paliogen® Red Violet L 5100 Color Additive Description: Quinacridone pigment especially for bordeaux and maroon shade Suitable for: Baking systems, Waterborn systems, Acrylic-isocyanate systems, and Airdrying systems.Information provided by .. |
|||
Electrical Resistivity | >= 5000 ohm-cm | >= 5000 ohm-cm | |
BASF Paliotan® Yellow L 2045 Color Additive Description: Pigment combination based on Bismuth VanadatSuitable for: Baking systems, Waterborn systems, Acrylic-isocyanate systems, Amine curing system and Airdrying systems.Information provided b.. |
|||
Electrical Resistivity | >= 5000 ohm-cm | >= 5000 ohm-cm | |
BASF Sicopal® Yellow L 1100 Color Additive Description: Weather-resistant inorganic bismuth vanadate pigment with high hiding power Chemical Structure: Bismuth vanadatSuitable for: Baking System, Waterborn systems, Acrylic-isocyanate systems.. |
|||
Electrical Resistivity | >= 5000 ohm-cm | >= 5000 ohm-cm | |
BASF Sicotan® Red L 2818 Color Additive Description: Transparent red iron oxideChemical Structure: Iron-III-OxideSuitable for: Baking System, Waterborn systems, Acrylic-isocyanate systems, Acid curing system, Amine curing system and Airdr.. |
|||
Electrical Resistivity | >= 5000 ohm-cm | >= 5000 ohm-cm | |
BASF Heligoen® Blue L 6900 Color Additive Description: Standard-a-phthalocyanine blues for economic formulations (L 6920 is somewhat stronger than L 6900).Chemical Structure: Cu-phthalocyanine, alpha-stabPhysical form: PowderSuitable for: B.. |
|||
Electrical Resistivity | >= 5000 ohm-cm | >= 5000 ohm-cm | |
BASF Heligoen® Blue L 6975 F Color Additive Description: Brilliant a-phthalocyanine blue with high color strength and excellent rheology in systems containing aromatic solventsChemical Structure: Cu-phthalocyanine, alpha-stabPhysical form: Po.. |
|||
Electrical Resistivity | >= 5000 ohm-cm | >= 5000 ohm-cm | |
BASF Heligoen® Blue L 7460 Color Additive Description: Metal free a-phthalocyanine blue especially for effect shadesChemical Structure: Cu-phthalocyanine, alpha-stab Physical form: PowderSuitable for: Baking systems, Waterborn systems, Acry.. |