Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 4.44e+13 ohm-cm | 4.44e+13 ohm-cm | |
Arkema Group Pebax® MX 1059 Polyether Block Amide (PEBA) (Dry) POLYETHER BLOCK AMIDE (PEBA) Hardness 35 shore D Good resistance to oils. Applications: Automotive, cable...ISO data provided by the manufacturer, Arkema. |