Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 3.00e+11 ohm-cm | 3.00e+11 ohm-cm | ASTM D257 |
Rogers Corporation Poron® 4701-30-15 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h.. |
|||
Electrical Resistivity | 3.00e+11 ohm-cm | 3.00e+11 ohm-cm | ASTM D257 |
Rogers Corporation Poron® 4701-30-20 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h.. |
|||
Electrical Resistivity | 3.00e+11 ohm-cm | 3.00e+11 ohm-cm | ASTM D257 |
Rogers Corporation Poron® 4701-30-30 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability test MVSS 302. Passes fogging test SAE-J 1736 for 3 hrs. at 100°C (212°F). Passes cold flexibility per MIL-P-12420D at -4.. |
|||
Electrical Resistivity | 3.00e+11 ohm-cm | 3.00e+11 ohm-cm | ASTM D257 |
Plenco 5314 Black (COM) Impact Grade Phenolic Molding Compound
(discontinued **) Plaslok 5314 is the replacement material for the former Union Carbide BMMA-5314. It is a two-stage, impact grade phenolic molding compound suitable for compression, transfer or injection molding of.. |
|||
Electrical Resistivity | 3.00e+11 ohm-cm | 3.00e+11 ohm-cm | ASTM D257 |
Plenco 5314 Black (INJ) Impact Grade Phenolic Molding Compound
(discontinued **) Plaslok 5314 is the replacement material for the former Union Carbide BMMA-5314. It is a two-stage, impact grade phenolic molding compound suitable for compression, transfer or injection molding of.. |
|||
Electrical Resistivity | 3.00e+11 ohm-cm | 3.00e+11 ohm-cm | ASTM D257 |
Plaslok 5314 Black (COM) Impact Grade Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 5314 is the replacement material for .. |
|||
Electrical Resistivity | 3.00e+11 ohm-cm | 3.00e+11 ohm-cm | ASTM D257 |
Plaslok 5314 Black (INJ) Impact Grade Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 5314 is the replacement material for .. |
|||
Electrical Resistivity | 3.00e+11 - 3.00e+12 ohm-cm | 3.00e+11 - 3.00e+12 ohm-cm | Average value: 1.39e+12 ohm-cm Grade Count:5 |
Overview of materials for Phenolic, Novolac, Mineral/Cellulose Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Cellulose Filled". Each property range of values reported is minimum and maxi.. |