Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 2.30e+15 ohm-cm | 2.30e+15 ohm-cm | |
3M Fluorinert™ FC-70 Electronic Liquid Fluorinert™ Liquid FC-70 a non-conductive, thermally and chemically stable liquid that offers a high boiling point (215 deg C), it is ideal for many electronics single and two phase heat transfer a.. |