Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.00e+8 - 2.00e+17 ohm-cm | 1.00e+8 - 2.00e+17 ohm-cm | Average value: 1.62e+16 ohm-cm Grade Count:173 |
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25.. |
|||
Electrical Resistivity | 1.00e+8 - 1.00e+15 ohm-cm @Temperature 66.0 - 130 °C |
1.00e+8 - 1.00e+15 ohm-cm @Temperature 151 - 266 °F |
Average value: 7.80e+13 ohm-cm Grade Count:7 |
Overview of materials for Epoxy, Cast, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Unreinforced". Each property range of values reported is minimum and maximum values of appr.. |
|||
Electrical Resistivity | 1.00e+8 - 5.80e+15 ohm-cm @Temperature 30.0 - 400 °C |
1.00e+8 - 5.80e+15 ohm-cm @Temperature 86.0 - 752 °F |
Average value: 1.21e+15 ohm-cm Grade Count:7 |
Overview of materials for Epoxy Encapsulant, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Encapsulant, Unreinforced". Each property range of values reported is minimum and maximum values o.. |
|||
Electrical Resistivity | 1.00e+8 - 1.00e+15 ohm-cm | 1.00e+8 - 1.00e+15 ohm-cm | Average value: 7.50e+14 ohm-cm Grade Count:11 |
Overview of materials for Nylon 6, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ.. |
|||
Electrical Resistivity | 1.00e+8 - 1.00e+15 ohm-cm | 1.00e+8 - 1.00e+15 ohm-cm | Average value: 8.57e+14 ohm-cm Grade Count:7 |
Overview of materials for Nylon 66, 10% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Mineral Filled". Specific grades with primary filler content between 5% and 14% are includ.. |
|||
Electrical Resistivity | <= 1.00e+8 ohm-cm | <= 1.00e+8 ohm-cm | |
Magyar Aluminum ALOLT 60F Aluminum Hydroxide Fine Precipitated Type |
|||
Electrical Resistivity | 1.00e+8 - 1.00e+12 ohm-cm | 1.00e+8 - 1.00e+12 ohm-cm | undoped |
Mateck Zinc Sulphide, ZnS Semiconductor single crystals. Twins and stacking faults < 4% of hexagonal phase. |
|||
Electrical Resistivity | 1.00e+8 - 1.00e+12 ohm-cm | 1.00e+8 - 1.00e+12 ohm-cm | |
BACT Dylyn® Diamond-Like Nanocomposite Coating a-C:H/a-Si:O nanocomposite. This coating provides the lowest friction of the BACT products, even in high humidity or wet environments. It offers an excellent combination of anti-stick and wear be.. |
|||
Electrical Resistivity | 1.00e+8 ohm-cm @Temperature 600 °C |
1.00e+8 ohm-cm @Temperature 1110 °F |
|
Anderman Ceramics EA998 Sintered Alumina, 99.8% High purity fully dense alumina (99.8%) with high temperature capability of 1750°C. Available in rod, tube, plate, crucibles, sheaths and insulators up to 10 ft (3 m) long with diameters 0.3" to 1.. |
|||
Electrical Resistivity | 1.00e+8 - 1.00e+15 ohm-cm | 1.00e+8 - 1.00e+15 ohm-cm | Average value: 3.02e+14 ohm-cm Grade Count:14 |
Overview of materials for Nylon 46, Flame Retarded + Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Flame Retarded + Glass Fiber Reinforced". Each property range of values reported is minimum an.. |
|||
Electrical Resistivity | 1.00e+8 - 1.00e+17 ohm-cm | 1.00e+8 - 1.00e+17 ohm-cm | Average value: 1.90e+15 ohm-cm Grade Count:64 |
Overview of materials for Nylon 6, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v.. |
|||
Electrical Resistivity | 1.00e+8 - 9.90e+10 ohm-cm | 1.00e+8 - 9.90e+10 ohm-cm | Average value: 2.02e+10 ohm-cm Grade Count:6 |
Overview of materials for Acrylic/Polycarbonate Alloy This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy". Each property range of values reported is minimum and maximum values of ap.. |
|||
Electrical Resistivity | 1.00e+8 - 1.00e+12 ohm-cm | 1.00e+8 - 1.00e+12 ohm-cm | undoped |
Mateck Zinc Selenide, ZnSe Semiconductor single crystals. Twins and stacking faults twin free. |