Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.00e+7 - 1.50e+16 ohm-cm @Temperature 75.0 - 300 °C |
1.00e+7 - 1.50e+16 ohm-cm @Temperature 167 - 572 °F |
Average value: 3.36e+15 ohm-cm Grade Count:2 |
Overview of materials for Epoxy Cure Resin This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Cure Resin". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Electrical Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | |
MarkeTech Gallium Arsenide Semiconductor Wafer, Semi-Insulating Chromium Doped, LEC Grown Data provided by the supplier, MarkeTech International.These materials are epi ready and are also available as polycrystal wafers and as seed crystals. Standard orientation: ±20' or 2-3° of .. |
|||
Electrical Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | |
MarkeTech Gallium Arsenide Semiconductor Wafer, Semi-Insulating Undoped, LEC Grown Data provided by the supplier, MarkeTech International.These materials are epi ready and are also available as polycrystal wafers and as seed crystals. Standard orientation: ±20' or 2-3° of .. |
|||
Electrical Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | |
MarkeTech Indium Phosphide Semiconductor Wafer, Semi-Insulating Iron Doped, Czochralski-LEC Grown Data provided by the supplier, MarkeTech International.These materials are epi ready and are also available as polycrystal wafers and as seed crystals. Standard orientation: ±20' or 2-3° of .. |
|||
Electrical Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | |
Ceradyne CeraTrex™ 146-3E Silicon Carbide Features:high puritycorrosion resistancewear resistancetailored electrical properties Applications:semiconductor componentssputtering targetsballistic armorwear componentsInformation provided by Cer.. |
|||
Electrical Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Algoflon® 15GR PTFE; Graphite Filled
(discontinued **) Data provided by the manufacturer.15 wt.% Graphite. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectric properties, almost n.. |
|||
Electrical Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Algoflon® 60BZ PTFE; Bronze Filled
(discontinued **) Data provided by the manufacturer.60 wt.% Bronze. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectric properties, almost no .. |
|||
Electrical Resistivity | 1.00e+7 - 1.00e+14 ohm-cm | 1.00e+7 - 1.00e+14 ohm-cm | Average value: 4.32e+13 ohm-cm Grade Count:7 |
Overview of materials for Nylon 46, Lubricated + Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Lubricated + Glass Fiber Reinforced". Each property range of values reported is minimum and ma.. |
|||
Electrical Resistivity | 1.00e+7 - 1.20e+17 ohm-cm | 1.00e+7 - 1.20e+17 ohm-cm | Average value: 1.80e+16 ohm-cm Grade Count:26 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported.. |