Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | <= 1.00e+6 ohm-cm | <= 1.00e+6 ohm-cm | IEC 60093 |
Murtfeldt Material ”S”® 1000 Black Antistatic Polyethylene, Conductive Material ”S”® 1000 is exclusively produced from ultra-high molecular weight polyethylene powder that is mixed with finely milled Original Material ”S”®. The fine milled material is compressio.. |
|||
Electrical Resistivity | >= 1.00e+6 ohm-cm | >= 1.00e+6 ohm-cm | IEC 60093 |
Murtfeldt Muralen® Black Antistatic Polyethylene, Conductive Muralen® is based on high molecular weight polyethylene (PE-HMW) and is ideally suited for use in applications that require the generally impressive material properties of polyethylene. Because of.. |
|||
Electrical Resistivity | <= 1.00e+6 ohm-cm | <= 1.00e+6 ohm-cm | IEC 60093 |
Murtfeldt Original Material ”S”® Black Antistatic Polyethylene, Conductive Original Material ”S”® black has the same properties as Original Material ”S”® green/natural. In addition, it is also electrostatically conductive due to the addition of additives. Special Pro.. |
|||
Electrical Resistivity | <= 1.00e+6 ohm-cm | <= 1.00e+6 ohm-cm | IEC 93 |
Quadrant EPP Cestlite™ ASTL Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |
|||
Electrical Resistivity | 1.00e+6 - 1.00e+17 ohm-cm | 1.00e+6 - 1.00e+17 ohm-cm | Average value: 9.89e+15 ohm-cm Grade Count:55 |
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% .. |
|||
Electrical Resistivity | 1.00e+6 ohm-cm | 1.00e+6 ohm-cm | IEC 60093 |
3M Dyneon™ TF 4215 PTFE 25% Electrocarbon Filled
(discontinued **) Applications include bearings, seals/gaskets, packings, piston rings.Data provided by Dyneon. |
|||
Electrical Resistivity | 1.00e+6 ohm-cm | 1.00e+6 ohm-cm | undoped |
Mateck Zinc Telluride, ZnTe Semiconductor single crystals. Twins and stacking faults twin free. |
|||
Electrical Resistivity | 1.00e+6 ohm-cm | 1.00e+6 ohm-cm | Specific Resistance |
UBE Tyranno Grade A Ceramic Semi-Conductive Fiber Description: Tyranno Fiber is the continuous ceramic fiber consisting of Si, Ti or Zr,C and O. Advanced composites reinforced by the Tyranno Fiber are expected to play a very important role in the e.. |
|||
Electrical Resistivity | 1.00e+6 ohm-cm @Temperature 1000 °C |
1.00e+6 ohm-cm @Temperature 1830 °F |
ASTM D1829 |
CoorsTek AD-96 Alumina (nom. 96% Al2O3) Thermal Shock Delta Tc = 250°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Electrical Resistivity | >= 1.00e+6 ohm-cm | >= 1.00e+6 ohm-cm | ASTM D1829 |
CoorsTek Pure SiC™ HR CVD Silicon Carbide, > 99.9995% Data Provided by the manufacturer, CoorsTek, Inc. |
|||
Electrical Resistivity | 1.00e+6 ohm-cm @Temperature 1000 °C |
1.00e+6 ohm-cm @Temperature 1830 °F |
ASTM D1829 |
CoorsTek Zirconia-Toughened Alumina, ZTA Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Electrical Resistivity | >= 1.00e+6 ohm-cm | >= 1.00e+6 ohm-cm | |
Dow Hydroxyethyl Acrylate Hydroxethyl Acrylate for high performance coatings. (Clear, colorless liquid)Information provided by Dow |
|||
Electrical Resistivity | >= 1.00e+6 ohm-cm | >= 1.00e+6 ohm-cm | |
Dow Hydroxypropyl Acrylate Hydroxypropyl Acrylate for high performance coatings. (Clear, colorless liquid)Information provided by Dow |
|||
Electrical Resistivity | >= 1.00e+6 ohm-cm | >= 1.00e+6 ohm-cm | |
Dow Glycidyl Methacrylate Glycidyl Methacrylate For Aliphatic Epoxy Polymers (Clear, colorless liquid)Information provided by Dow |
|||
Electrical Resistivity | 1.00e+6 ohm-cm @Temperature 600 °C |
1.00e+6 ohm-cm @Temperature 1110 °F |
|
Anderman Ceramics EM60P Sillimanite Porous synthetic mullite with high thermal shock. Available as tube up to 10 ft (3 m) long with diameters 0.6" to 2.4".Information provided by Anderman Ceramics. |
|||
Electrical Resistivity | 1.00e+6 ohm-cm @Temperature 600 °C |
1.00e+6 ohm-cm @Temperature 1110 °F |
|
Anderman Ceramics EM80P Corundum Porous synthetic mullite with very high thermal shock. Available as tube, sheath, or rod up to 10 ft (3 m) long with diameters 0.3" to 20".Information provided by Anderman Ceramics. |
|||
Electrical Resistivity | 1.00e+6 ohm-cm | 1.00e+6 ohm-cm | |
Ceradyne CeraTrex™ 146-IS Silicon Carbide Features:high puritycorrosion resistancewear resistanceApplications:semiconductor componentssputtering targetsInformation provided by Ceradyne Company |
|||
Electrical Resistivity | 1.00e+6 - 1.00e+12 ohm-cm | 1.00e+6 - 1.00e+12 ohm-cm | |
BACT DLC Diamond-Like Coating DLC (a-C:H). This coating provides the highest hardness and abrasion resistance of the BACT products. Typical applications include high wear environments involving seals, molds, metal forming, and.. |
|||
Electrical Resistivity | 1.00e+6 ohm-cm @Temperature 600 °C |
1.00e+6 ohm-cm @Temperature 1110 °F |
|
Anderman Ceramics EM60 Mullite Synthetic mullite available in rod, tube, sheaths and insulators up to 10 ft (3 m) long with diameters 0.3" to 19".Information provided by Anderman Ceramics. |
|||
Electrical Resistivity | 1.00e+6 - 1.00e+18 ohm-cm | 1.00e+6 - 1.00e+18 ohm-cm | Average value: 3.44e+16 ohm-cm Grade Count:35 |
Overview of materials for Low Density Polyethylene (LDPE), Wire/Cable Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Wire/Cable Grade". Each property range of values reported is minimum an.. |
|||
Electrical Resistivity | 1.00e+6 ohm-cm | 1.00e+6 ohm-cm | |
Ceradyne CeraTrex™ 146-S5 Silicon Carbide Features:corrosion resistancewear resistancehardnessnet shape fabricationApplications:wear componentsInformation provided by Ceradyne Company |