Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | >= 1.00e+14 ohm-cm | >= 1.00e+14 ohm-cm | dry; IEC 60093 |
Murtfeldt Murylon® B Nylon 6 Murylon® B natural has the best impact resistance of all Murylon materials. This material is especially suited for use in machine construction thanks to an excellent combination of mechanical prope.. |
|||
Electrical Resistivity | >= 1.00e+14 ohm-cm | >= 1.00e+14 ohm-cm | dry; IEC 60093 |
Murtfeldt Murytal® H Acetal Homopolymer In addition to the excellent properties of Murytal® C, Murytal® H is stronger and more rigid with a lower expansion coefficient.Special Properties:• High rigidity• Excellent ability to regain it.. |
|||
Electrical Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ASTM D257 |
Rogers Corporation Bisco™ HT-820 Cellular Silicone Foam Firm grade silicone sponge. UL recognized for flame retardance.Applications: Gaskets where higher closure force is available or necessary, Cushions in heavier-load applicationsGasketing and sealing.. |
|||
Electrical Resistivity | >= 1.00e+14 ohm-cm | >= 1.00e+14 ohm-cm | dry; IEC 60093 |
Murtfeldt Murylat® Polyethylene Terephthalate Thanks to its extremely low absorption of moisture and low expansion coefficient, Murylat® is ideally suited for the processing of precision parts. Murylat® has an extremely high hardness grade an.. |
|||
Electrical Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ASTM D257 |
Shell Carilon® DB6F0A10 Polyketone, Flame-Retarded (V-0) Injection Molding Grade
(discontinued **) Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer DB6F0A10 is a flame-retarded injection molding grade with mechanical properties which classify it a.. |
|||
Electrical Resistivity | 1.00e+14 - 2.20e+16 ohm-cm | 1.00e+14 - 2.20e+16 ohm-cm | Average value: 8.01e+15 ohm-cm Grade Count:8 |
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler". Specific grades with glass content between 15%.. |
|||
Electrical Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ISO data |
BASF Capron® 5233G 33% Glass-Filled Nylon 66 (Dry)
(discontinued **) Capron 5233G is a 33% glass fiber reinforced, polyamide 6,6 injection molding compound offering excellent strength, stiffness, creep resistance and dimensional stability. This balance of engineerin.. |
|||
Electrical Resistivity | 1.00e+14 - 1.00e+16 ohm-cm | 1.00e+14 - 1.00e+16 ohm-cm | |
Kraton® D1116 (SB)n Branched Copolymer (SB)n - styrene-butadiene multi-arm (branched) copolymer. KRATON® Polymers require no premastication or vulcanization. They can be blended with thermoplastic polymers and significantly improve .. |
|||
Electrical Resistivity | 1.00e+14 - 1.00e+16 ohm-cm | 1.00e+14 - 1.00e+16 ohm-cm | |
Kraton® D4141 (SBS) Linear Block Copolymer (SBS) styrene-butadiene-styrene block polymer. KRATON® Polymers require no premastication or vulcanization. They can be blended with thermoplastic polymers and significantly improve the impact .. |
|||
Electrical Resistivity | 1.00e+14 ohm-cm @Temperature 25.0 °C |
1.00e+14 ohm-cm @Temperature 77.0 °F |
|
Goodfellow Ruby, Al2O3 Ruby exhibits identical properties to those of sapphire. Small amounts of impurities, especially chromium oxide, give ruby a red coloration. Useful optical range from 150 - 5500 nm.Information pro.. |
|||
Electrical Resistivity | >= 1.00e+14 ohm-cm | >= 1.00e+14 ohm-cm | ASTM D1829 |
CoorsTek AD-85 Alumina (nom. 85% Al2O3) Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Electrical Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | |
Arkema Group Rilsan® ARVO 950 TLD Nylon 12, Rotomolding Grade (Conditioned) Designation ISO 1874-PA12,RHLR,16-010Grade for rotomolding. Available color: natural. Light and heat stabilized. Mold-release agent.Easy to be processed in the same conditions as polyethylene. High .. |
|||
Electrical Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | |
Arkema Group Rilsan® BECN W3 TL Nylon 11, Sheathing Grade (Conditioned) Designation ISO 1874-PA11,KFHL,12-010Rigid grade for sheathing wires and cables. Available color: natural. Light and heat stabilized. Flame retardant agent.Fire-resistant. High abrasion resistance. .. |
|||
Electrical Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | |
Arkema Group Rilsan® Powder T NAT BHV COS Nylon 11, Cosmetic Grade Powder T NAT BHV COS - RILSAN POLYAMIDE 11 (PA11) POWDERUnpigmented and clear Powder for the cosmetic industry, used as mild abrasive in 'scrubbing' creams.The properties listed in the dat.. |
|||
Electrical Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | |
BASF Novolen® 2348 M Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Electrical Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | |
BASF Novolen® 2448 L Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Electrical Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ASTM D257 |
Ashley Polymers Ashlene® 527LDS-B2 Nylon 66 A high impact lubricated nylon resin containing well dispersed carbon black for maximum resistance to weathering.Data provided by the manufacturer |
|||
Electrical Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | IEC 60093 |
CENTROPLAST CENTRO HPM Polysulfone This plastic has good hydrolysis, chemical and radiation resistance, and can operate at high temperatures. It is used in food processing industry, pumps and valves, and medical equipment.Informatio.. |
|||
Electrical Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | IEC 60093 |
CENTROPLAST CENTROMID 6.6 GF 30 Polyamide 6.6 30% glass fiber This material has very high strength and rigidity, with lower moisture absorption. It can be used for housing parts, threaded bolts, and distance pieces.Information provided by CENTROPLAST Engineer.. |
|||
Electrical Resistivity | 1.00e+14 - 1.00e+15 ohm-cm | 1.00e+14 - 1.00e+15 ohm-cm | Minimum |
Ceradyne Ceralloy® 147-31E Sintered Reaction Bonded Silicon Nitride (Si3N4) Ceralloy® 147 Reaction Bonded Silicon Nitride (RBSN) is a high purity grade of silicon nitride. RBSN has excellent thermal shock resistance and outstanding compatibility with non-ferrous molten met.. |
|||
Electrical Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ASTM D257 |
Ashley Polymers Ashlene® 79MGS Nylon 6, 40% Glass Mineral reinforced A 40% glass mineral reinforced Nylon 6 with good dimensional stability, stiffness, sink and warp resistance. Modified for improved surface appearance.Data provided by the manufacturer |
|||
Electrical Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | |
Anderman Ceramics EA998 Sintered Alumina, 99.8% High purity fully dense alumina (99.8%) with high temperature capability of 1750°C. Available in rod, tube, plate, crucibles, sheaths and insulators up to 10 ft (3 m) long with diameters 0.3" to 1.. |
|||
Electrical Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | Volume; GB1410 |
Beijing Evergrow Resources Glass Filled Nylon Information provided by Beijing Evergrow Resources. |
|||
Electrical Resistivity | 1.00e+14 - 1.00e+15 ohm-cm | 1.00e+14 - 1.00e+15 ohm-cm | Average value: 7.00e+14 ohm-cm Grade Count:15 |
Overview of materials for Acrylic, Impact Modified, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified, Molded". Each property range of values reported is minimum and maximum values .. |