Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | >= 1.00e+13 ohm-cm | >= 1.00e+13 ohm-cm | 50% RH; IEC 60093 |
Murtfeldt Murylon® A GF Nylon 66, Glass Reinforced Murylon® A’s impressive characteristics are enhanced with admixed glass fibers. This results in a clear improvement in cold flow behavior and dimensional stability, enabling higher static pressure.. |
|||
Electrical Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | ASTM D257 |
Shell Carilon® DP R1130 Polyketone, 30% Glass Fiber Reinforced
(discontinued **) Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON® Thermoplastic Polymer DP R1130 is a 30 percent glass fiber reinforced compound based on a developmental e.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | Average value: 5.50e+14 ohm-cm Grade Count:27 |
Overview of materials for Acetal Homopolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values .. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+17 ohm-cm | 1.00e+13 - 1.00e+17 ohm-cm | Average value: 4.52e+16 ohm-cm Grade Count:12 |
Overview of materials for Polycarbonate, Optical Grade This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
Eastman Tenite Butyrate 513E3720008 Clear, Trsp Cellulose Acetate Butyrate
(discontinued **) Plasticizer 23%. Weight loss on heating = 1.2% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | Average value: 8.50e+13 ohm-cm Grade Count:6 |
Overview of materials for Nylon 612, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Electrical Resistivity | >= 1.00e+13 ohm-cm | >= 1.00e+13 ohm-cm | |
MarkeTech AN 90 Aluminum Nitride Ceramic Substrate, 98% Purity Data provided by the supplier, MarkeTech International.Substrate Specs: Maximum dimensions 5.5 x 3.6 in.. Thickness 0.12-0.60 in. Surface roughness 0.3 µm as fired; 0.075 µm lapped; 0.025 Â.. |
|||
Electrical Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | IEC 93 |
Solvay Technyl® A 218 V35 Nylon 66, 35% Glass Fiber, EH50 Polyamides PA66, reinforced with 35% of glass fiber, heat stabilized, for injection molding.Technyl A 218 V35 is used in all sectors of industry, offering an excellent combination between thermal an.. |
|||
Electrical Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | IEC 93 |
Solvay Technyl® A 246M Nylon 66, Impact Grade, EH50 Unreinforced and modified polyamide 66, with improved impact resistance, heat stabilized, for injection molding.Technyl A 246m offers an excellent notched impact resistance at low temperatures makin.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
Eastman Tenite Acetate 105E1R26033 Clear, Trsp Cellulose Acetate Plasticizer 29%. Weight loss on heating = 2.6% per ASTM D 707. Soluble matter loss = 0.4% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
Eastman Tenite Butyrate 485A2R30016 Natural Cellulose Acetate Butyrate Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.TENITE cellulosic plastics are noted for their excellent balance of properties - toughness,.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
Eastman Tenite Butyrate 550E4861316 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
Eastman Tenite Propionate 371A2R30009 Natural, Trsp Cellulose Acetate Propionate Plasticizer 9%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
Eastman Tenite Propionate 371A2R30012 Natural, Trsp Cellulose Acetate Propionate Plasticizer 18%. Weight loss on heating = 1% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pro.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
Eastman Tenite Propionate 381E4000015 Clear, Trsp Cellulose Acetate Propionate Plasticizer 15%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
Eastman Tenite Propionate 383A2R30009 Natural, Trsp Cellulose Acetate Propionate Plasticizer 9%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Electrical Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | |
Dow Tyrin® 3623A Chlorinated Polyethylene Elastomer 36% Chlorine. Tyrin® chlorinated polyethylene thermoplastic resins offer the compounding and fabrication industries end product properties in a range of hardnesses, and behave much like flexible P.. |
|||
Electrical Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | |
Dow Tyrin® CM2136P Chlorinated Polyethylene Elastomer 36% Chlorine. Tyrin® chlorinated polyethylene thermoplastic resins offer the compounding and fabrication industries end product properties in a range of hardnesses, and behave much like flexible P.. |
|||
Electrical Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | ASTM D257 |
Chang Chun Plastic Longlite PM T310 Impact Phenolic Molding Compound ASTM Grade per ASTM D700 is 13.Information provided by Dowell Trading Company Ltd. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
Eastman Tenite Butyrate 465A3720010 Clear, Trsp Cellulose Acetate Butyrate
(discontinued **) Plasticizer 10%. Weight loss on heating = 0.9% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
Eastman Tenite Propionate 350E0096914 Natural, Trsp Cellulose Acetate Propionate Plasticizer 12%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
Eastman Tenite Butyrate 581A3720016 Clear, Trsp Cellulose Acetate Butyrate
(discontinued **) Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |