Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.00e+11 - 4.00e+16 ohm-cm | 1.00e+11 - 4.00e+16 ohm-cm | Average value: 1.05e+15 ohm-cm Grade Count:72 |
Overview of materials for Polyester Thermoplastic Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values.. |
|||
Electrical Resistivity | 1.00e+11 - 1.00e+17 ohm-cm | 1.00e+11 - 1.00e+17 ohm-cm | Average value: 6.50e+15 ohm-cm Grade Count:36 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is .. |
|||
Electrical Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | IEC 60093 |
3M Dyneon™ TF 4303 PTFE 15% Graphite Filled
(discontinued **) Type II PTFE. Applications include sliding surfaces, bearings, seals/gaskets.Data provided by Dyneon. |
|||
Electrical Resistivity | 1.00e+11 - 1.00e+15 ohm-cm | 1.00e+11 - 1.00e+15 ohm-cm | Average value: 2.88e+14 ohm-cm Grade Count:12 |
Overview of materials for Nylon 66/6, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are incl.. |
|||
Electrical Resistivity | 1.00e+11 - 1.00e+15 ohm-cm | 1.00e+11 - 1.00e+15 ohm-cm | Average value: 6.50e+14 ohm-cm Grade Count:8 |
Overview of materials for Nylon 66, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Extruded". Each property range of values reported is minimum and maximum values of appropriate.. |
|||
Electrical Resistivity | 1.00e+11 - 1.00e+17 ohm-cm | 1.00e+11 - 1.00e+17 ohm-cm | Average value: 9.59e+15 ohm-cm Grade Count:19 |
Overview of materials for Nylon 66, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are inclu.. |
|||
Electrical Resistivity | 1.00e+11 - 1.00e+16 ohm-cm @Temperature 20.0 - 500 °C |
1.00e+11 - 1.00e+16 ohm-cm @Temperature 68.0 - 932 °F |
|
MarkeTech Sapphire (Aluminum Oxide - Al2O3) Single Crystal Data provided by the supplier, MarkeTech International.Sapphire is grown by several methods: Boule form (Czochralski), in plate form, or as tubes, rods and plates. Boules are grown up to 8" diam.. |
|||
Electrical Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | IEC 93 |
Solvay Technyl® C 216 Nylon 6, 30% Glass Fiber, EH50 Polyamide PA6, reinforced with 30% of glass fiber, for injection molding.It has good mechanical properties. It is used in all sectors of industry, offering an excellent combination between thermal .. |
|||
Electrical Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | |
Sapco C 410 Steatite Information provided by Sapco. |
|||
Electrical Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | |
Sapco C 220 Steatite Information provided by Sapco. |
|||
Electrical Resistivity | 1.00e+11 ohm-cm @Temperature 500 °C |
1.00e+11 ohm-cm @Temperature 932 °F |
ASTM D1829 |
CoorsTek PlasmaPure™ Alumina (nom. 99.8% Al2O3) Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Electrical Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | |
Arkema Group Rilsan® AMN P30 LD Nylon 12, Flexible, Injection Grade (Conditioned) Designation ISO 1874-PA12-P,MLR,12-004Flexible grade for injection molding. Available color: black. Light stabilized. Mold-release agent.Good impact strength. Flexibility and dynamic properties. Eas.. |
|||
Electrical Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | |
Arkema Group Rilsan® AMN P40 TLD Nylon 12, Flexible, Injection Grade (Conditioned) Designation ISO 1874-PA12-P,MHLR,14-004Flexible grade for injection molding. Available colors: black and natural. Light and heat stabilized. Mold-release agent.Good impact strength. Flexibility and .. |
|||
Electrical Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | |
Arkema Group Rilsan® BESN P40 TL Nylon 11, Flexible Tubing Grade (Conditioned) Designation ISO 1874-PA11-P,EHL,22-003Flexible grade for tubes extrusion. Available color: black and natural. Light and heat stabilized.High flexibility. High impact strength. Very good chemical res.. |
|||
Electrical Resistivity | >= 1.00e+11 ohm-cm | >= 1.00e+11 ohm-cm | DIN 53482/VDE 0303 |
BASF Elastollan® C-95A Polyester Type Polyurethane Elastomer Processed by extrusion or injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellen.. |
|||
Electrical Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | ASTM D257 |
Chang Chun Plastic Longlite PM T308J General Purpose Phenolic Molding Compound ASTM Grade per ASTM D700 is 3.Information provided by Dowell Trading Company Ltd. |
|||
Electrical Resistivity | >= 1.00e+11 ohm-cm | >= 1.00e+11 ohm-cm | DIN 53482/VDE 0303 |
BASF Elastollan® 1195A Polyether Type Polyurethane Elastomer Processed by extrusion or injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes... |
|||
Electrical Resistivity | 1.00e+11 ohm-cm @Temperature 65.0 °C |
1.00e+11 ohm-cm @Temperature 149 °F |
Insulation Resistance During 10th day Cycling (95% Relative Humidity) |
Cytec Conathane® CE-1163 (Conap) Polyurethane Dielectric Conformal Coating Dielectric Conformal Coatings for ElectronicsCytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, i.. |
|||
Electrical Resistivity | 1.00e+11 - 1.00e+14 ohm-cm | 1.00e+11 - 1.00e+14 ohm-cm | Average value: 1.63e+13 ohm-cm Grade Count:22 |
Overview of materials for Melamine-Phenolic Copolymer This property data is a summary of similar materials in the MatWeb database for the category "Melamine-Phenolic Copolymer". Each property range of values reported is minimum and maximum values of ap.. |