Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00400 ohm-cm | 0.00400 ohm-cm | |
Poco Graphite SUPERSiC® 3C Silicon Carbide SUPERSiC that has been coated with a 75 µm CVD SiC coating, which seals the surface.Uses: Ideal for high-temperature deposition and CVD applications.Information provided by PocoGraphite |
|||
Electrical Resistivity | 0.00400 ohm-cm | 0.00400 ohm-cm | |
Poco Graphite SUPERSiC® 3CX Silicon Carbide SUPERSiC that has been coated twice with a 75 µm CVD SiC coating, which seals the surface. Uses: Ideal for high-temperature anneal processesInformation provided by PocoGraphite |
|||
Electrical Resistivity | 0.00400 ohm-cm | 0.00400 ohm-cm | |
Poco Graphite SUPERSiC® Si-3C Silicon Carbide SUPERSiC that has been infiltrated with silicon and then coated with a 75 µm CVD SiC coating, sealing off the porosity.Uses: Ideal for high-temperature vacuum CVD systemsInformation provided by Poc.. |
|||
Electrical Resistivity | 0.00400 - 0.00700 ohm-cm | 0.00400 - 0.00700 ohm-cm | |
Alliance BIN-40 Bonded (Composite) Magnetic Material |
|||
Electrical Resistivity | 0.00400 - 0.00700 ohm-cm | 0.00400 - 0.00700 ohm-cm | |
Alliance BIN-26 Bonded (Composite) Magnetic Material |
|||
Electrical Resistivity | 0.00400 - 0.00700 ohm-cm | 0.00400 - 0.00700 ohm-cm | |
Alliance BIN-45 Bonded (Composite) Magnetic Material |
|||
Electrical Resistivity | 0.00400 - 0.00700 ohm-cm | 0.00400 - 0.00700 ohm-cm | |
Alliance BIN-48 Bonded (Composite) Magnetic Material |
|||
Electrical Resistivity | 0.00400 - 0.00700 ohm-cm | 0.00400 - 0.00700 ohm-cm | |
Alliance BIN-55 Bonded (Composite) Magnetic Material |
|||
Electrical Resistivity | 0.00400 - 0.00700 ohm-cm | 0.00400 - 0.00700 ohm-cm | |
Alliance BIN-72 Bonded (Composite) Magnetic Material |
|||
Electrical Resistivity | 0.00400 ohm-cm | 0.00400 ohm-cm | |
Poco Graphite SUPERSiC® Si-8C Silicon Carbide SUPERSiC that has been infiltrated with silicon and then coated with a 200 µm CVD SiC coatingUses: Ideal for optical and lithography componentsInformation provided by Poco Graphite |