Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00120 ohm-cm | 0.00120 ohm-cm | Dried Coating after DMSO addition |
Heraeus Cleviosâ„¢ PH 1000 Conductive Sulfonate Polymer for Antistatic Coatings Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ PH 1000 is an antistatic material based on PED.. |
|||
Electrical Resistivity | 0.00120 ohm-cm | 0.00120 ohm-cm | |
UCAR Carbon UCAR® ATR Isostatic Molded Graphite Isostatically molded ATR is a lower density version of grade ATJ. It is a fine grain, high strength material which can be machined to precise tolerances and a fine surface finish.Typical Application.. |
|||
Electrical Resistivity | 0.00120 ohm-cm | 0.00120 ohm-cm | Filament |
Cytec Thornel® Mat VMA Carbon Fiber Data provided by the manufacturer, Amoco Performance Products, Inc.Composed of high strength, high modulus carbon filaments in a random-layered orientation. The fine diameter filaments are up to th.. |
|||
Electrical Resistivity | 0.00120 ohm-cm | 0.00120 ohm-cm | Filament |
Cytec Thornel® Mat VMC Carbon Fiber Data provided by the manufacturer, Amoco Performance Products, Inc.Prepared by sectioning mat VMA into cubes ~ 0.5x0.5x1.0 in. VMC can be heterogeneously dispersed in matrix materials and thus enha.. |
|||
Electrical Resistivity | 0.00120 ohm-cm | 0.00120 ohm-cm | Filament |
Cytec Thornel® Mat VMD Carbon Fiber Data provided by the manufacturer, Amoco Performance Products, Inc.Form of mat VMA with shorter fibers for injection molding. Fiber lengths average 400 µm - adequate for good property improvement... |
|||
Electrical Resistivity | 0.00120 ohm-cm | 0.00120 ohm-cm | Filament |
Cytec Thornel® Mat VME Carbon Fiber Data provided by the manufacturer, Amoco Performance Products, Inc.Form of mat VMA with shorter fibers for injection molding. Fiber lengths average 200 µm - inadequate for good mechanical property.. |