Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0001245 ohm-cm @Temperature 800 °C |
0.0001245 ohm-cm @Temperature 1470 °F |
|
Haynes HR-120® alloy, solution heat-treated Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Electrical Resistivity | 0.0001245 ohm-cm @Temperature 800 °C |
0.0001245 ohm-cm @Temperature 1470 °F |
|
Haynes HR-120® alloy, solution heat-treated aged at 1200°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Electrical Resistivity | 0.0001245 ohm-cm @Temperature 800 °C |
0.0001245 ohm-cm @Temperature 1470 °F |
|
Haynes HR-120® alloy, solution heat-treated aged at 1400°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Electrical Resistivity | 0.0001245 ohm-cm @Temperature 800 °C |
0.0001245 ohm-cm @Temperature 1470 °F |
|
Haynes HR-120® alloy, solution heat-treated aged at 1600°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Electrical Resistivity | 0.0001245 ohm-cm @Temperature 800 °C |
0.0001245 ohm-cm @Temperature 1470 °F |
|
Haynes HR-120® alloy, solution heat-treated aged at 1800°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Electrical Resistivity | 0.0001245 ohm-cm @Temperature 900 °C |
0.0001245 ohm-cm @Temperature 1650 °F |
|
Haynes HR-160® alloy plate, aged 1000 hours at 649°C (1200°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Electrical Resistivity | 0.0001245 ohm-cm @Temperature 900 °C |
0.0001245 ohm-cm @Temperature 1650 °F |
|
Haynes HR-160® alloy plate, aged 4000 hours at 649°C (1200°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Electrical Resistivity | 0.0001245 ohm-cm @Temperature 900 °C |
0.0001245 ohm-cm @Temperature 1650 °F |
|
Haynes HR-160® alloy, annealed plate Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Electrical Resistivity | 0.0001245 ohm-cm @Temperature 900 °C |
0.0001245 ohm-cm @Temperature 1650 °F |
|
Haynes HR-160® alloy, hot rolled and solution annealed plate Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Electrical Resistivity | 0.0001245 ohm-cm @Temperature 900 °C |
0.0001245 ohm-cm @Temperature 1650 °F |
|
Haynes HR-160® alloy, plate, aged 1000 hours at 760°C (1400°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Electrical Resistivity | 0.0001245 ohm-cm @Temperature 900 °C |
0.0001245 ohm-cm @Temperature 1650 °F |
|
Haynes HR-160® alloy, plate, aged 1000 hours at 871°C (1600°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Electrical Resistivity | 0.0001245 ohm-cm @Temperature 900 °C |
0.0001245 ohm-cm @Temperature 1650 °F |
|
Haynes HR-160® alloy, plate, aged 4000 hours at 760°C (1400°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Electrical Resistivity | 0.0001245 ohm-cm @Temperature 900 °C |
0.0001245 ohm-cm @Temperature 1650 °F |
|
Haynes HR-160® alloy, plate, aged 4000 hours at 871°C (1600°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Electrical Resistivity | 0.0001245 ohm-cm @Temperature 900 °C |
0.0001245 ohm-cm @Temperature 1650 °F |
|
Haynes HR-160® alloy, plate, aged 8000 hours at 760°C (1400°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Electrical Resistivity | 0.0001245 ohm-cm @Temperature 900 °C |
0.0001245 ohm-cm @Temperature 1650 °F |
|
Haynes HR-160® alloy, plate, aged 8000 hours at 871°C (1600°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Electrical Resistivity | 0.0001245 ohm-cm @Temperature 900 °C |
0.0001245 ohm-cm @Temperature 1650 °F |
|
Haynes HR-160® alloy, solution annealed sheet Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Electrical Resistivity | 0.0001245 ohm-cm @Temperature 800 °C |
0.0001245 ohm-cm @Temperature 1470 °F |
|
Haynes HR-120® alloy, solution heat-treated plate Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Electrical Resistivity | 0.0001245 ohm-cm @Temperature 900 °C |
0.0001245 ohm-cm @Temperature 1650 °F |
|
Haynes HR-160® alloy plate, aged 8000 hours at 649°C (1200°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |