Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000820 ohm-cm | 0.0000820 ohm-cm | |
Crucible Steel XM-19 Stainless Steel Crucible XM-19 Stainless is a nitrogen strengthened, low carbon, austenitic, stainless steel that provides good corrosion resistance in combination with high strength. The alloy has better corrosio.. |
|||
Electrical Resistivity | 0.0000820 ohm-cm | 0.0000820 ohm-cm | |
Carlson Nitronic® 50® Austenitic Stainless Steel General DescriptionNitronic 50 is a nitrogen-strengthened austenitic stainless steel that possesses corrosion resistance superior to 316, 316L, 317 and 317L plus approximately twice the yield streng.. |
|||
Electrical Resistivity | 0.0000820 ohm-cm | 0.0000820 ohm-cm | Temperature Coefficient = 0.0011 |
Carpenter Invar 36® Alloy, Annealed Bars and Strip Data provided by Carpenter Technology Corporation.Carpenter Invar "36" alloy is a 36% nickel-iron alloy possessing a rate of thermal expansion approx. one-tenth that of carbon steel up to 200°C. T.. |
|||
Electrical Resistivity | 0.0000820 ohm-cm | 0.0000820 ohm-cm | Temperature Coefficient = 0.0011 |
Carpenter Invar 36® Alloy, Cold Drawn Bars Data provided by Carpenter Technology Corporation.Carpenter Invar "36" alloy is a 36% nickel-iron alloy possessing a rate of thermal expansion approx. one-tenth that of carbon steel up to 200°C. T.. |
|||
Electrical Resistivity | 0.0000820 ohm-cm | 0.0000820 ohm-cm | Temperature Coefficient = 0.0011 |
Carpenter Invar 36® Alloy, Cold Rolled Strip Data provided by Carpenter Technology Corporation.Carpenter Invar "36" alloy is a 36% nickel-iron alloy possessing a rate of thermal expansion approx. one-tenth that of carbon steel up to 200°C. T.. |
|||
Electrical Resistivity | 0.0000820 ohm-cm | 0.0000820 ohm-cm | |
AK Steel 17-7 PH® Precipitation Hardening Stainless Steel, Condition TH 1050 AK Steel 17-7 PH® provides high strength and hardness, excellent fatigue properties, good corrosion resistance, good formability, and minimum distortion upon heat treatment. This alloy provides va.. |