Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000600 ohm-cm | 0.0000600 ohm-cm | RT |
Outokumpu 4016 Ferritic Stainless Steel Fairly good corrosion resistant formable steel in mildly corrosive environments. Oxidation resistant at elevated temperatures (up to ~800°C). Ductile, does not work harden readily, and is well su.. |
|||
Electrical Resistivity | 0.0000600 ohm-cm @Temperature 20.0 °C |
0.0000600 ohm-cm @Temperature 68.0 °F |
|
Industeel SOLEIL A2 13% Cr High Strength Martensitic Stainless Steel (QT550 Heat Treatment) Description: Soleil A2 has combined Chromium (~13%) and Carbon ~0.10%) additions to provide an excellent combination of high mechanical properties and improved corrosion resistance properties. The g.. |
|||
Electrical Resistivity | 0.0000600 ohm-cm | 0.0000600 ohm-cm | |
Special Metals NILOMAG® Alloy 77 A nickel-iron alloy with additions of copper and molybdenum. It is a low-loss, soft-magnetic alloy with a high initial permeability. Initial permeability 60,000; maximum permeability 300,000; satu.. |
|||
Electrical Resistivity | 0.0000600 ohm-cm | 0.0000600 ohm-cm | |
TIMET 75A CP Titanium (ASTM Grade 4) Commercially Pure Titanium. Industry Specifications: USA Aerospace: AMS 4901. Germany Engineering: 3.7065. Germany Aerospace: 3.7064. France: T-60. UK Aerospace Specification BS TA. 6.Features.. |
|||
Electrical Resistivity | 0.0000600 ohm-cm @Temperature 23.0 °C |
0.0000600 ohm-cm @Temperature 73.4 °F |
|
Crucible Steel 440B Chromium Steel Crucible 440B Is a hardenable chromium steel which is cutlery grade having high attainable hardness and toughness. This grade is magnetic at all times. Information provided by Crucible Specialty Me.. |
|||
Electrical Resistivity | 0.0000600 ohm-cm | 0.0000600 ohm-cm | |
ETREMA Products Terfenol-D Magnetostrictive Smart Material (Tb0.3Dy0.7Fe1.92) Terfenol-D is the commercial name for Tb0.3Dy0.7Fe1.92; a composition of material that exhibits giant magnetostriction.Magnetostriction is the phenomenon in which an applied magnetic field causes an.. |
|||
Electrical Resistivity | 0.0000600 ohm-cm | 0.0000600 ohm-cm | |
Bohler-Uddeholm BÖHLER S401(M1) High Speed Steel Description: Molybdenum high speed steel with high toughness and good cutting ability. Applications: Taps, twist drills, reamers, milling tools, broaches toolsStandards: DIN/EN 1.3346 HS2-91, AISI M.. |
|||
Electrical Resistivity | 0.0000600 ohm-cm | 0.0000600 ohm-cm | |
AK Steel 400 Ferritic Stainless steel AK Steel 400 is one of the most economical chromium ferritic stainless steels. It has corrosion and oxidation resistance comparable to Type 410 stainless steel with good fabricating characteristics.. |
|||
Electrical Resistivity | 0.0000600 ohm-cm | 0.0000600 ohm-cm | |
AK Steel 409 Ferritic Stainless steel AK Steel 409 Stainless Steels are especially useful for applications where oxidation or corrosion protection beyond the capacity of carbon steel and some coated steels is needed. Current applicatio.. |
|||
Electrical Resistivity | 0.0000600 ohm-cm | 0.0000600 ohm-cm | |
AK Steel 409 ULTRA FORM® Stainless Steel AK Steel 409 ULTRA FORM Stainless Steel provides an outstanding combination of improved forming and welding characteristics, while providing superior resistance to oxidation, corrosion, ridging and .. |
|||
Electrical Resistivity | 0.0000600 ohm-cm | 0.0000600 ohm-cm | |
AK Steel 410S Ferritic Stainless steel AK Steel 410S Stainless Steel is a non-hardening modification of Type 410. A small titanium addition minimizes austenite formation at high temperatures, thereby restricting the alloy's ability to h.. |
|||
Electrical Resistivity | 0.0000600 ohm-cm | 0.0000600 ohm-cm | |
AK Steel 430 Ferritic Stainless steel AK Steel 430 combines good corrosion resistance and heat and oxidation resistance up to 1500°F with good mechanical properties. Typical consumer applications include automotive trim and molding, f.. |
|||
Electrical Resistivity | 0.0000600 ohm-cm | 0.0000600 ohm-cm | |
AK Steel 430 ULTRA FORM® Stainless Steel 430 ULTRA FORM® Stainless Steel was developed as a more formable version of Type 430 stainless steel. It is particularly suited for parts requiring more complex shapes. 430 ULTRA FORM Stainless Ste.. |
|||
Electrical Resistivity | 0.0000600 ohm-cm | 0.0000600 ohm-cm | |
AK Steel 434 Ferritic Stainless steel AK Steel 434 is a modification of Type 430, the addition of molybdenum increases this alloy's corrosion resistance and its attack from many deicing chemicals. It also provides good heat and oxidati.. |
|||
Electrical Resistivity | 0.0000600 ohm-cm | 0.0000600 ohm-cm | 409 HP™ |
ATI Allegheny Ludlum AL 409 Cb™ Brazeable Ferritic Stainless Steel, 14% Cold Work AL 409 Cb™ is normally 12.5% chromium ferritic stainless steel with columbium stabilization and with restricted titanium and aluminum contents. As a result of these alloying adjustments, the braze.. |
|||
Electrical Resistivity | 0.0000600 ohm-cm | 0.0000600 ohm-cm | 409 HP™ |
ATI Allegheny Ludlum AL 409 Cb™ Brazeable Ferritic Stainless Steel, 16.4% Cold Work AL 409 Cb™ is normally 12.5% chromium ferritic stainless steel with columbium stabilization and with restricted titanium and aluminum contents. As a result of these alloying adjustments, the braze.. |
|||
Electrical Resistivity | 0.0000600 ohm-cm | 0.0000600 ohm-cm | 409 HP™ |
ATI Allegheny Ludlum AL 409 Cb™ Brazeable Ferritic Stainless Steel, 2.9% Cold Work AL 409 Cb™ is normally 12.5% chromium ferritic stainless steel with columbium stabilization and with restricted titanium and aluminum contents. As a result of these alloying adjustments, the braze.. |
|||
Electrical Resistivity | 0.0000600 ohm-cm | 0.0000600 ohm-cm | 409 HP™ |
ATI Allegheny Ludlum AL 409 Cb™ Brazeable Ferritic Stainless Steel, 34.5% Cold Work AL 409 Cb™ is normally 12.5% chromium ferritic stainless steel with columbium stabilization and with restricted titanium and aluminum contents. As a result of these alloying adjustments, the braze.. |
|||
Electrical Resistivity | 0.0000600 ohm-cm | 0.0000600 ohm-cm | 409 HP™ |
ATI Allegheny Ludlum AL 409 Cb™ Brazeable Ferritic Stainless Steel, 43.6% Cold Work AL 409 Cb™ is normally 12.5% chromium ferritic stainless steel with columbium stabilization and with restricted titanium and aluminum contents. As a result of these alloying adjustments, the braze.. |
|||
Electrical Resistivity | 0.0000600 ohm-cm | 0.0000600 ohm-cm | 409 HP™ |
ATI Allegheny Ludlum AL 409 Cb™ Brazeable Ferritic Stainless Steel, 8.5% Cold Work AL 409 Cb™ is normally 12.5% chromium ferritic stainless steel with columbium stabilization and with restricted titanium and aluminum contents. As a result of these alloying adjustments, the braze.. |
|||
Electrical Resistivity | 0.0000600 ohm-cm | 0.0000600 ohm-cm | |
ATI Allegheny Ludlum AL 409HP™ Ferritic Stainless Steel, UNS S40930 Type 409 ferritic stainless steel was introduced by Allegheny Ludlum in 1961 to provide improved oxidation and corrosion resistance for automotive exhaust systems in comparison to carbon automotive .. |
|||
Electrical Resistivity | 0.0000600 ohm-cm | 0.0000600 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel AL 410S™ (UNS S41008) Allegheny Ludlum Al 410S™ stainless steel is a low-carbon modification of Type 410 stainless steel. Low carbon and optionally a small addition of titanium and /or columbium minimize austenite form.. |
|||
Electrical Resistivity | 0.0000600 ohm-cm | 0.0000600 ohm-cm | 409 HP™ |
ATI Allegheny Ludlum AL 409 Cb™ Brazeable Ferritic Stainless Steel, 20% Cold Work AL 409 Cb™ is normally 12.5% chromium ferritic stainless steel with columbium stabilization and with restricted titanium and aluminum contents. As a result of these alloying adjustments, the braze.. |
|||
Electrical Resistivity | 0.0000600 ohm-cm | 0.0000600 ohm-cm | 409 HP™ |
ATI Allegheny Ludlum AL 409 Cb™ Brazeable Ferritic Stainless Steel AL 409 Cb™ is normally 12.5% chromium ferritic stainless steel with columbium stabilization and with restricted titanium and aluminum contents. As a result of these alloying adjustments, the braze.. |
|||
Electrical Resistivity | 0.0000600 ohm-cm @Temperature 20.0 °C |
0.0000600 ohm-cm @Temperature 68.0 °F |
|
Industeel SOLEIL A2 13% Cr High Strength Martensitic Stainless Steel (QT650 Heat Treatment) Description: Soleil A2 has combined Chromium (~13%) and Carbon ~0.10%) additions to provide an excellent combination of high mechanical properties and improved corrosion resistance properties. The g.. |