Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000547 ohm-cm | 0.0000547 ohm-cm | |
Special Metals MONEL® Alloy 400 A nickel-copper alloy with high strength and excellent corrosion resistance in a range of media including sea water, hydrofluoric acid, sulfuric acid, and alkalis. Used for marine engineering, chem.. |