Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000370 ohm-cm | 0.0000370 ohm-cm | |
Indium Corp. Indalloy® 10 Pb-In Solder Alloy Indalloy's #7, #10, #150, #204, #205 and #206 comprise a group of lead-indium solders designed to cover the temperature range of 165°C-275°C. All have the minimum gold-leaching characteristics.. |
|||
Electrical Resistivity | 0.0000370 ohm-cm | 0.0000370 ohm-cm | |
Bohler-Uddeholm BÖHLER M261 Extra Plastic Lens Mold Steel VACUUM ARC REMELTED HARDENED AND TEMPERED PLASTIC LENS MOLD STEELBOHLER M261 follow current trends in tool and die-making:Excellent machinability coupled with higher hardnessGood dimensional stabili.. |
|||
Electrical Resistivity | 0.0000370 ohm-cm | 0.0000370 ohm-cm | Fully Processed and Semi-Processed |
AK Steel DI-MAX® M-45 Nonoriented Electrical Steel Nonoriented electrical steels are silicon steels in which magnetic properties are practically the same in any direction of magnetism in the plane of the material. Standard
grades from M-15 to M-47 .. |
|||
Electrical Resistivity | 0.0000370 ohm-cm | 0.0000370 ohm-cm | Fully Processed and Semi-Processed |
AK Steel DI-MAX® M-47 Nonoriented Electrical Steel Nonoriented electrical steels are silicon steels in which magnetic properties are practically the same in any direction of magnetism in the plane of the material. Standard
grades from M-15 to M-47 .. |