Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000230 ohm-cm | 0.0000230 ohm-cm | |
CLAL-MSX NICLAL 1300 0 Annealed Copper Alloy, Free Cutting Nickel-Silver Main Characteristics: Good ductilityGood corrosion resistanceTypical Applications:High volume turned partsKeysInformation provided by CLAL-MSX |
|||
Electrical Resistivity | 0.0000230 ohm-cm | 0.0000230 ohm-cm | |
CLAL-MSX NICLAL 1300 H12 1/2 Hard Copper Alloy, Free Cutting Nickel-Silver Main Characteristics: Good ductilityGood corrosion resistanceTypical Applications:High volume turned partsKeysInformation provided by CLAL-MSX |
|||
Electrical Resistivity | 0.0000230 ohm-cm | 0.0000230 ohm-cm | |
CLAL-MSX NICLAL 1300 H14 4/4 Hard Copper Alloy, Free Cutting Nickel-Silver Main Characteristics: Good ductilityGood corrosion resistanceTypical Applications:High volume turned partsKeysInformation provided by CLAL-MSX |