Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000137 ohm-cm | 0.0000137 ohm-cm | |
Indium Corp. Indalloy 132 Tin Solder Alloy High temperature electrical solderInformation Provided by Indium Corporation |
|||
Electrical Resistivity | 0.0000137 ohm-cm | 0.0000137 ohm-cm | Annealed |
Eagle Brass 521 Phosphor Bronzes 8% C, 1/2 Hard Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical.. |
|||
Electrical Resistivity | 0.0000137 ohm-cm | 0.0000137 ohm-cm | Annealed |
Eagle Brass 521 Phosphor Bronzes 8% C, 1/4 Hard Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical.. |
|||
Electrical Resistivity | 0.0000137 ohm-cm | 0.0000137 ohm-cm | Annealed |
Eagle Brass 521 Phosphor Bronzes 8% C, 3/4 Hard Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical.. |
|||
Electrical Resistivity | 0.0000137 ohm-cm | 0.0000137 ohm-cm | Annealed |
Eagle Brass 521 Phosphor Bronzes 8% C, Annealed Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical.. |
|||
Electrical Resistivity | 0.0000137 ohm-cm | 0.0000137 ohm-cm | Annealed |
Eagle Brass 521 Phosphor Bronzes 8% C, Extra Hard Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical.. |
|||
Electrical Resistivity | 0.0000137 ohm-cm | 0.0000137 ohm-cm | Annealed |
Eagle Brass 521 Phosphor Bronzes 8% C, Extra Spring Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical.. |
|||
Electrical Resistivity | 0.0000137 ohm-cm | 0.0000137 ohm-cm | Annealed |
Eagle Brass 521 Phosphor Bronzes 8% C, Hard Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical.. |
|||
Electrical Resistivity | 0.0000137 ohm-cm | 0.0000137 ohm-cm | Annealed |
Eagle Brass 521 Phosphor Bronzes 8% C, Spring Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical.. |