Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000110 ohm-cm | 0.0000110 ohm-cm | |
Hogen HM3000 Tungsten-Based Metal Mil Spec T-21014D Class 3; ASTM B-777-99 Class 3; AMS T-21014 Class 3. Nil magnetic properties.Manufactured by powder metallurgy methods. The tungsten base offers high thermal conductivity and a l.. |
|||
Electrical Resistivity | 0.0000110 ohm-cm | 0.0000110 ohm-cm | |
Indium Corp. Indalloy 128 Pure Tin Information Provided by Indium Corporation |
|||
Electrical Resistivity | 0.0000110 ohm-cm | 0.0000110 ohm-cm | |
Indium Corp. Indalloy® 121 Sn-Ag Solder Alloy Binary solder has history of use, marginal wetting. Standard tin-silver eutectic solder with wide application when lead-based solders do not meet temperature, strength or safety requirements. Not r.. |
|||
Electrical Resistivity | 0.0000110 ohm-cm | 0.0000110 ohm-cm | |
Mi-Tech Metals HD18 Tungsten-Based Metal Mil Spec T-21014D Class 3; ASTM B-777-99 Class 3; ASTM B-777-07 Class 3; AMS T-21014 Class 3. Nil magnetic properties.Manufactured by powder metallurgy methods. The tungsten base offers high therm.. |
|||
Electrical Resistivity | 0.0000110 ohm-cm | 0.0000110 ohm-cm | |
Indium Corp. Indalloy® 201 Sn-Zn Solder Alloy Recommended for soldering to aluminum. Use flux #3. Zn causes high drossing, short shelf life as solder paste.Information provided by the manufacturer, Indium Corporation. |
|||
Electrical Resistivity | 0.0000110 ohm-cm | 0.0000110 ohm-cm | |
Williams Advanced Alloys WS232 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Electrical Resistivity | 0.0000110 - 0.0000160 ohm-cm | 0.0000110 - 0.0000160 ohm-cm | Temperature Coefficient of 0.0006 to 0.0007/K |
Goodfellow Phosphor Bronze Good Machinability. Uses include springs, clips, gauzes and architectural applicationsInformation provided by Goodfellow. |