Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000960 ohm-cm | 0.00000960 ohm-cm | |
Lucas-Milhaupt BRAZE 452 Characteristics:Braze 452 is a free-flowing, low temperature filler metal commonly used to replace cadmium-bearing filler metals of similar silver content. This alloy is best suited for narrow gap .. |
|||
Electrical Resistivity | 0.00000960 ohm-cm | 0.00000960 ohm-cm | |
Lucas-Milhaupt Silvaloy® A34T Brazing Alloy Silvaloy A34T is used for joining ferrous metals, copper, copper alloys, nickel, nickel alloys and combinations of these metals. The tin content provides good wetting on many difficult wet metals su.. |
|||
Electrical Resistivity | 0.00000960 ohm-cm | 0.00000960 ohm-cm | |
Lucas-Milhaupt Silvaloy® A40T Brazing Alloy Silvaloy A40T is a good general purpose, low melting, cadmium-free alloy, often selected for its low temperature, wetting and good flow. Silvaloy A40T has a lower brazing temperature with a relative.. |
|||
Electrical Resistivity | 0.00000960 ohm-cm | 0.00000960 ohm-cm | |
Lucas-Milhaupt Silvaloy® A45T Brazing Alloy Silvaloy A45T is a free flowing, low melting and an excellent substitute to the cadmium bearing filler metals with similar silver contents. Silvaloy A45T narrow melt range makes it suitable for manu.. |
|||
Electrical Resistivity | 0.00000960 ohm-cm | 0.00000960 ohm-cm | |
Special Metals Nickel 200 Commercially pure (99.6%) wrought nickel with good mechanical properties and resistance to a range of corrosive media. Good thermal, electrical, and magnetostrictive properties. Ferromagnetic. Us.. |
|||
Electrical Resistivity | 0.00000960 ohm-cm | 0.00000960 ohm-cm | 18 % IACS |
CMW® ELKALOY D Copper Alloy, Aluminum Bronze ELKALOY® D alloys are aluminum bronze type casting alloys. The sequence, ELKALOY® D, D110, D120, D130 materials represents increasing hardness and abrasion resistance but reduced electrical and th.. |
|||
Electrical Resistivity | 0.00000960 ohm-cm | 0.00000960 ohm-cm | |
Lucas-Milhaupt BRAZE 402 Silver Based Cadmium Free Filler Metal Characteristics: Braze 402 is a free-flowing, intermediate temperature filler metal and as such is a good substitute for cadmium-bearing filler metals with similar silver contents. The material is .. |