Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000539 ohm-cm | 0.00000539 ohm-cm | (32% IACS) |
CMW® THERMKON® 70M Molybdenum Copper parts For matching CTE of semiconductor substrates while allowing high thermal transfer.Information provided by CMW Inc. |