Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000280 ohm-cm | 0.00000280 ohm-cm | 62 % IACS |
CMW® ELKONITE 4050 tungsten, high silver ELKONITE® 4050 is a high silver material that uses a special tungsten powder. It is made by the press-sinter-infiltrate method. It was developed especially for use as a combination current carrying.. |