Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.100 - 25.0 ohm-cm | 0.100 - 25.0 ohm-cm | |
MarkeTech Silicon Single Crystal Semiconductor Wafer, n-type, Phosphorous Doped, Czochralski-LED Grown Data provided by the supplier, MarkeTech International.MarkeTech International supplies standard silicon single crystals grown with diameters from 51 to 150 mm from polycrystal material with donor c.. |