Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.00e+11 - 2.00e+15 ohm-cm | 1.00e+11 - 2.00e+15 ohm-cm | Average value: 2.79e+14 ohm-cm Grade Count:13 |
Overview of materials for Nylon 11, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |