Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.00 - 10.0 ohm-cm | 1.00 - 10.0 ohm-cm | ASTM D257 |
PolyOne Stat-Tech™ AS-7SS/000 ABS - 7% Stainless Steel Fiber
(discontinued **) Data provided by PolyOne. |
|||
Electrical Resistivity | 0.100 - 10.0 ohm-cm | 0.100 - 10.0 ohm-cm | Average value: 5.39 ohm-cm Grade Count:4 |
Overview of materials for Nylon 11 + Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 + Carbon Fiber". Each property range of values reported is minimum and maximum values of approp.. |
|||
Electrical Resistivity | 1.00 - 10.0 ohm-cm | 1.00 - 10.0 ohm-cm | ASTM C611 |
Techmer ES Electrafil® DB-5/SS/10 Polycarbonate, 10% Stainless Steel Fiber (dry blend) |
|||
Electrical Resistivity | 1.00 - 10.0 ohm-cm | 1.00 - 10.0 ohm-cm | ASTM C611 |
Techmer ES Electrafil® J-1/CF/30 Nylon 66, 30% Carbon Fiber Reinforced Carbon Fiber Reinforced |
|||
Electrical Resistivity | 1.00 - 10.0 ohm-cm | 1.00 - 10.0 ohm-cm | ASTM C611 |
Techmer ES Electrafil® J-1/CF/30/TF/13/SI/2 Nylon 66, 30% Carbon Fiber, 13% PTFE, 2% Silicone |
|||
Electrical Resistivity | 1.00 - 10.0 ohm-cm | 1.00 - 10.0 ohm-cm | ASTM C611 |
Techmer ES Electrafil® J-1/CF/30/TF/15 Nylon 66, 30% Carbon Fiber Reinforced, PTFE Lubed Carbon Fiber Reinforced, PTFE Lubricated |
|||
Electrical Resistivity | 1.00 - 10.0 ohm-cm | 1.00 - 10.0 ohm-cm | ASTM C611 |
Techmer ES Electrafil® J-3/CF/30 Nylon 6, 30% Carbon Fiber Reinforced |
|||
Electrical Resistivity | 1.00 - 10.0 ohm-cm | 1.00 - 10.0 ohm-cm | ASTM C611 |
Techmer ES Electrafil® J-50/CF/40 Polycarbonate, 40% Carbon Fiber Reinforced, PTFE Lubricated |
|||
Electrical Resistivity | 1.00 - 10.0 ohm-cm | 1.00 - 10.0 ohm-cm | |
A. Schulman ComAlloy E-16903B Nylon 6/6, Electrically Conductive - Stainless Steel Fiber Filled Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Electrical Resistivity | 1.00 - 10.0 ohm-cm | 1.00 - 10.0 ohm-cm | |
A. Schulman ComAlloy E-16901B PPS Alloy, Electrically Conductive - Carbon Fiber Filled Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Electrical Resistivity | 1.00 - 10.0 ohm-cm | 1.00 - 10.0 ohm-cm | |
A. Schulman ComAlloy E-16902N PPS Alloy, Electrically Conductive - Stainless Steel Fiber Filled Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Electrical Resistivity | 0.100 - 10.0 ohm-cm | 0.100 - 10.0 ohm-cm | Average value: 6.70 ohm-cm Grade Count:3 |
Overview of materials for Polyphenylene Sulfide (PPS), NCG Fiber This property data is a summary of similar materials in the MatWeb database for the category "PPS + NGG". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |