Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 100 - 1.20e+17 ohm-cm | 100 - 1.20e+17 ohm-cm | Average value: 8.69e+15 ohm-cm Grade Count:110 |
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim.. |
|||
Electrical Resistivity | 1.00e+7 - 1.20e+17 ohm-cm | 1.00e+7 - 1.20e+17 ohm-cm | Average value: 1.80e+16 ohm-cm Grade Count:26 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported.. |