Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1000 - 1.00e+18 ohm-cm | 1000 - 1.00e+18 ohm-cm | Average value: 2.51e+16 ohm-cm Grade Count:75 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |
|||
Electrical Resistivity | 1000 - 1.00e+18 ohm-cm | 1000 - 1.00e+18 ohm-cm | Average value: 1.25e+17 ohm-cm Grade Count:110 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
Electrical Resistivity | 1.00e+14 - 1.00e+18 ohm-cm | 1.00e+14 - 1.00e+18 ohm-cm | Average value: 2.90e+17 ohm-cm Grade Count:28 |
Overview of materials for Polystyrene, Heat Resistant Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Heat Resistant Grade". Each property range of values reported is minimum and maximum values.. |
|||
Electrical Resistivity | 1.00e+14 - 1.00e+18 ohm-cm | 1.00e+14 - 1.00e+18 ohm-cm | Average value: 2.27e+17 ohm-cm Grade Count:9 |
Overview of materials for Polystyrene, Transparent Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Transparent Grade". Each property range of values reported is minimum and maximum values of.. |
|||
Electrical Resistivity | 1.00e+14 - 1.00e+18 ohm-cm | 1.00e+14 - 1.00e+18 ohm-cm | Average value: 1.11e+17 ohm-cm Grade Count:70 |
Overview of materials for Polycarbonate, UV Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a.. |
|||
Electrical Resistivity | 100 - 1.00e+18 ohm-cm | 100 - 1.00e+18 ohm-cm | Average value: 1.42e+16 ohm-cm Grade Count:81 |
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i.. |
|||
Electrical Resistivity | 10000 - 1.00e+18 ohm-cm | 10000 - 1.00e+18 ohm-cm | Average value: 1.87e+17 ohm-cm Grade Count:44 |
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Glass Filled, Molded". Each property range of values reported is minimum.. |
|||
Electrical Resistivity | 1.00e+17 - 1.00e+18 ohm-cm | 1.00e+17 - 1.00e+18 ohm-cm | Average value: 8.94e+17 ohm-cm Grade Count:17 |
Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyperfluoroalkoxyethylene, Molded/Extruded". Each property range of values reported is minimum and max.. |
|||
Electrical Resistivity | 1.00e+17 - 1.00e+18 ohm-cm | 1.00e+17 - 1.00e+18 ohm-cm | Average value: 9.55e+17 ohm-cm Grade Count:10 |
Overview of materials for Fluorinated Ethylene Propylene (FEP), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Fluorinated Ethylene Propylene (FEP), Molded/Extruded". Each property range of values reported is minimu.. |
|||
Electrical Resistivity | 100 - 1.00e+18 ohm-cm | 100 - 1.00e+18 ohm-cm | Average value: 7.19e+16 ohm-cm Grade Count:13 |
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler". Specific grades with glass content between 25%.. |
|||
Electrical Resistivity | 100 - 1.00e+18 ohm-cm | 100 - 1.00e+18 ohm-cm | Average value: 4.11e+16 ohm-cm Grade Count:70 |
Overview of materials for Nylon 66, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum .. |
|||
Electrical Resistivity | 1000 - 1.00e+18 ohm-cm | 1000 - 1.00e+18 ohm-cm | Average value: 3.64e+16 ohm-cm Grade Count:71 |
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma.. |
|||
Electrical Resistivity | 1.00e+6 - 1.00e+18 ohm-cm | 1.00e+6 - 1.00e+18 ohm-cm | Average value: 3.44e+16 ohm-cm Grade Count:35 |
Overview of materials for Low Density Polyethylene (LDPE), Wire/Cable Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Wire/Cable Grade". Each property range of values reported is minimum an.. |
|||
Electrical Resistivity | 1.00e+10 - 1.00e+18 ohm-cm | 1.00e+10 - 1.00e+18 ohm-cm | Average value: 1.68e+17 ohm-cm Grade Count:6 |
Overview of materials for Nylon 66, Nucleated This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Nucleated". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Electrical Resistivity | 1.00e+14 - 1.00e+18 ohm-cm | 1.00e+14 - 1.00e+18 ohm-cm | Average value: 1.33e+17 ohm-cm Grade Count:8 |
Overview of materials for Polystyrene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Extrusion Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
Electrical Resistivity | 1.00e+9 - 1.00e+18 ohm-cm | 1.00e+9 - 1.00e+18 ohm-cm | Average value: 1.28e+16 ohm-cm Grade Count:96 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+18 ohm-cm | 1.00e+13 - 1.00e+18 ohm-cm | Average value: 5.20e+16 ohm-cm Grade Count:22 |
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+18 ohm-cm | 1.00e+13 - 1.00e+18 ohm-cm | Average value: 6.01e+16 ohm-cm Grade Count:19 |
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% .. |
|||
Electrical Resistivity | 1000 - 1.00e+18 ohm-cm | 1000 - 1.00e+18 ohm-cm | Average value: 2.85e+17 ohm-cm Grade Count:14 |
Overview of materials for Polypropylene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Extrusion Grade". Each property range of values reported is minimum and maximum values of.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+18 ohm-cm | 1.00e+13 - 1.00e+18 ohm-cm | Average value: 3.76e+16 ohm-cm Grade Count:33 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum .. |