Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000910 - 0.0000100 ohm-cm | 0.00000910 - 0.0000100 ohm-cm | |
PEAK Werkstoff DISPAL S263 Aluminum Alloy, AlSi25Cu3Fe3Ni3MgCoTi, Condition T6 Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |
|||
Electrical Resistivity | 0.00000910 - 0.0000100 ohm-cm | 0.00000910 - 0.0000100 ohm-cm | |
PEAK Werkstoff DISPAL S263 Aluminum Alloy, AlSi25Cu3Fe3Ni3MgCoTi, Condition F Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |
|||
Electrical Resistivity | 0.00000910 - 0.0000100 ohm-cm | 0.00000910 - 0.0000100 ohm-cm | |
PEAK Werkstoff DISPAL S263 Aluminum Alloy, AlSi25Cu3Fe3Ni3MgCoTi, Condition T4 Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |