Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000810 - 0.00000880 ohm-cm | 0.00000810 - 0.00000880 ohm-cm | |
PEAK Werkstoff DISPAL S225 Aluminum Alloy, AlSi35Fe2Ni, Condition F Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |