Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 8.00e+12 - 4.20e+13 ohm-cm | 8.00e+12 - 4.20e+13 ohm-cm | Average value: 2.47e+13 ohm-cm Grade Count:3 |
Overview of materials for Phenolic, Resole, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Mineral Filled". Each property range of values reported is minimum and maximum values .. |
|||
Electrical Resistivity | 8.00e+12 - 1.00e+16 ohm-cm | 8.00e+12 - 1.00e+16 ohm-cm | Average value: 3.34e+15 ohm-cm Grade Count:3 |
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Elastomer, Unreinforced". Each property range of values reported is minimum and .. |