Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 7.00e+7 ohm-cm @Temperature 350 °C |
7.00e+7 ohm-cm @Temperature 662 °F |
|
Momentive Performance Materials Type 214 Fused Quartz Tubing Used for clear fused quartz lamp tubing. GE 214 is a high purity, high transmittance, high temperature material with a low hydroxyl (OH-) content. It is suitable for a broad range of mercury, halo.. |