Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 600 ohm-cm | 600 ohm-cm | 4.6% graphite |
TIMCAL TIMREX® KS15 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Electrical Resistivity | 600 ohm-cm | 600 ohm-cm | 4.2% graphite |
TIMCAL TIMREX® MB15 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Electrical Resistivity | 600 ohm-cm | 600 ohm-cm | |
Arkema Group Rilsan® ASR 20 Nylon 12, 20% Carbon Fiber Filled (Conditioned) Designation ISO 1874-PA12,M,16-090,CF20Rigid grade with carbon fiber filler (20%) for injection molding. Available color: black. High strength-to-weight ratio. Very low shrinkage: include 0,5% on av.. |