Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 5.00e+16 ohm-cm | 5.00e+16 ohm-cm | ASTM D257 |
Ensinger ENSIFONE® PSU (Polysulfone) - Extruded Products
(discontinued **) ENSIFONE is a transparent engineering plastic known for its chemical resistance, rigidity, high-temperature performance, and its ability to operate in an autoclave environment. ENSIFONE is FDA and .. |