Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 5.00e+14 ohm-cm | 5.00e+14 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Ryton® R-4-220BL Polyphenylene Sulfide Compound
(Unverified Data**) Black Polyphenylene Sulfide CompoundRyton® R-4-220BL is an advanced 40% fiberglass reinforced polyphenylene sulfide compound formulated for enhanced hydrolytic stability in applications requiring .. |
|||
Electrical Resistivity | 5.00e+14 ohm-cm | 5.00e+14 ohm-cm | IEC 93 |
Solvay Technyl® A 218 V30 Nylon 66, 30% Glass Fiber, EH0 Polyamide PA66, reinforced with 30% of glass fiber, heat stabilized, for injection molding.Technyl A 218 V30 is used in all sectors of industry, offering an excellent combination between thermal and.. |
|||
Electrical Resistivity | 5.00e+14 ohm-cm | 5.00e+14 ohm-cm | ASTM D257 |
Toyobo Pelprene™ P-280B Polyester TPE Key Feature: Pelprene P typePelprene™ can be processed into a wide variety of articles from ultra-small precision parts to sheets by injection, extrusion, and blow molding. The 'P' type is a block.. |
|||
Electrical Resistivity | 5.00e+14 ohm-cm | 5.00e+14 ohm-cm | ASTM D257 |
Toyobo Pelprene™ S-6001 Polyester TPE Key Feature: Pelprene S typePelprene™ can be processed into a wide variety of articles from ultra-small precision parts to sheets by injection, extrusion, and blow molding. The 'S' type is a block.. |
|||
Electrical Resistivity | 5.00e+14 ohm-cm | 5.00e+14 ohm-cm | |
Covestro Desmopan® 372 Thermoplastic Polyurethane Desmopan 372 is a TPU on the basis of a special ester.Applications: Transport rolls, technical automotive parts.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separa.. |
|||
Electrical Resistivity | 5.00e+14 ohm-cm | 5.00e+14 ohm-cm | ASTM D257 |
Ensinger ENSIKEM® PVDF (Polyvinylidene Fluoride) - Extruded Products
(discontinued **) Polyvinylidene fluoride, or PVDF, is a fluorinated thermoplastic resin that has outstanding resistance to most mineral and organic acids, aliphatic and aromatic hydrocarbons, alcohols, halogenated s.. |
|||
Electrical Resistivity | 5.00e+14 ohm-cm | 5.00e+14 ohm-cm | ASTM D257 |
Quantum Composites QC-8704 63% Glass Fiber Vinyl Ester SMC
(discontinued **) QC-8704 is a vinyl ester-based epoxy sheet molding compound (SMC) designed for compression and transfer molding of components requiring high structural strength. It exhibits unusual toughness, and .. |
|||
Electrical Resistivity | 5.00e+14 ohm-cm | 5.00e+14 ohm-cm | ASTM D257 |
Quantum Composites QC-8704FR 63% Glass Fiber Flame Retardant Vinyl Ester SMC
(discontinued **) QC-8704FR is a vinyl ester-based epoxy sheet molding compound (SMC) designed for compression and transfer molding of components requiring high structural strength. It exhibits unusual toughness, an.. |
|||
Electrical Resistivity | 5.00e+14 - 4.00e+16 ohm-cm | 5.00e+14 - 4.00e+16 ohm-cm | Average value: 7.72e+15 ohm-cm Grade Count:14 |
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and.. |
|||
Electrical Resistivity | 5.00e+14 - 1.00e+17 ohm-cm | 5.00e+14 - 1.00e+17 ohm-cm | Average value: 2.43e+16 ohm-cm Grade Count:24 |
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m.. |
|||
Electrical Resistivity | 5.00e+14 ohm-cm | 5.00e+14 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Ryton® R-4-220NA Polyphenylene Sulfide Compound
(Unverified Data**) Natural Color Polyphenylene Sulfide CompoundRyton® R-4-220NA is an advanced 40% fiberglass reinforced polyphenylene sulfide compound formulated for enhanced hydrolytic stability in applications re.. |