Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 430000 ohm-cm | 430000 ohm-cm | |
Arkema Group Orgalloy® RS 6030 AT Nylon 6 Alloy, 30% Glass Fiber (Conditioned) RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties... |