Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 4000 - 1.00e+17 ohm-cm | 4000 - 1.00e+17 ohm-cm | Average value: 6.60e+15 ohm-cm Grade Count:17 |
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar.. |
|||
Electrical Resistivity | 4000 - 300000 ohm-cm | 4000 - 300000 ohm-cm | Average value: 176000 ohm-cm Grade Count:8 |
Overview of materials for Nylon 6 Fiber This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6 Fiber". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Electrical Resistivity | 4000 - 1.00e+19 ohm-cm | 4000 - 1.00e+19 ohm-cm | Average value: 6.75e+16 ohm-cm Grade Count:139 |
Overview of materials for Nylon 66, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Electrical Resistivity | 4000 ohm-cm | 4000 ohm-cm | |
Shakespeare Resistat® F9216 F040 Nylon 66 Monofilament Resistat F2416, MERGE F040 is a nylon 6,6 multifilament yarn. Each filament has electrically conductive carbon suffused into the surface. The filaments have a round cross section with a coating th.. |
|||
Electrical Resistivity | 4000 ohm-cm | 4000 ohm-cm | |
Shakespeare Resistat® F9222 B040 Nylon 6 Monofilament Resistat F9222, MERGE B040 is a 22 denier per filament conductive nylon 6 tow. Each filament has electrically conductive carbon suffused into the surface. The filaments have a round cross section .. |