Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 300 ohm-cm | 300 ohm-cm | 4.9% graphite |
TIMCAL TIMREX® MK15 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Electrical Resistivity | 300 ohm-cm | 300 ohm-cm | 4.7% graphite |
TIMCAL TIMREX® MX15 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Electrical Resistivity | 300 ohm-cm | 300 ohm-cm | 4.9% graphite |
TIMCAL TIMREX® MX25 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |