Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.60e+14 ohm-cm | 1.60e+14 ohm-cm | |
Momentive Performance Materials RTV31 Red Extreme High Temperature Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Electrical Resistivity | 1.60e+14 ohm-cm | 1.60e+14 ohm-cm | |
Momentive Performance Materials RTV41 White General Purpose Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |