Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.56e+16 ohm-cm | 1.56e+16 ohm-cm | |
Solvay Specialty Polymers Halar® 300 ECTFE Fluoropolymer
(discontinued **) Data provided by the manufacturer.HALAR® Fluoropolymers have excellent barrier properties, high resistance to a variety of corrosive chemicals and solvents, low flammability, and ease of processing.. |
|||
Electrical Resistivity | 1.56e+16 ohm-cm | 1.56e+16 ohm-cm | |
Solvay Specialty Polymers Halar® 500 ECTFE Fluoropolymer
(discontinued **) Data provided by the manufacturer.HALAR® Fluoropolymers have excellent barrier properties, high resistance to a variety of corrosive chemicals and solvents, low flammability, and ease of processing.. |