Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.40e+17 ohm-cm | 1.40e+17 ohm-cm | per ASTM D257-91 |
DuPont™ Kapton® 300HN Polyimide Film, 75 Micron Thickness Film thickness 75 micron (3.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Available in thicknesses from 0.3 mil (7.5 µm) to 5 mil (125 µm).General.. |
|||
Electrical Resistivity | 1.40e+17 ohm-cm | 1.40e+17 ohm-cm | per ASTM D257-91 |
DuPont™ Kapton® 300VN Polyimide Film, 75 Micron Thickness Film thickness 75 micron (3.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type HN with added dimensional stability. Available i.. |
|||
Electrical Resistivity | 1.40e+17 ohm-cm | 1.40e+17 ohm-cm | |
DuPont™ Kapton® 120FN616 Polyimide/FEP Composite Film 120 Gauge film structure consisting of a 25 µm (1 mil) base polyimide film with a 2.5 µm (0.1 mil) coating of Teflon® FEP on both sides.Kapton® Type HN film coated with Teflon® FEP fluoropolyme.. |