Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.19e+16 ohm-cm | 1.19e+16 ohm-cm | |
Abatron AboCast 50-11/AboCure 50-12 Epoxy Information provided by Abatron, Inc.Processing: Shelf life: 12+ months (unmixed). 100/13.5 ratio. Pot life: 500 g, 36 min. at 25°C (77°F). Exothermic Peak 265°C (510°F). Hardens in 2-24 hou.. |
|||
Electrical Resistivity | >= 1.19e+16 ohm-cm | >= 1.19e+16 ohm-cm | |
Abatron AboCast 50-16/AboCure 50-12 Epoxy Information provided by Abatron, Inc.Processing: Shelf life: 12+ months (unmixed). 100/14 ratio. Pot life: 500 g, 38 min. at 25°C (77°F). Exothermic Peak 280°C (535°F). Hardens in 2-24 hours.. |