Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.00e+16 - 2.10e+17 ohm-cm | 1.00e+16 - 2.10e+17 ohm-cm | Average value: 9.11e+16 ohm-cm Grade Count:9 |
Overview of materials for Polyaryletherketone (PAEK), Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Glass Fiber Filled". Each property range of values reported is minimum and m.. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
Plenco 50240 PET, Pellet, Injection Molded, Natural Color
(discontinued **) PLENCO 50240 is an engineering grade glass reinforced UL flame rated polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in natural and black.. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
PolyOne Edgetek® ES-15GF/000 RED Polyethersulfone - 15% Glass Fiber Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
PolyOne Edgetek® ES-40GF/000 Polyethersulfone - 40% Glass Fiber Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Electrical Resistivity | >= 1.00e+16 ohm-cm | >= 1.00e+16 ohm-cm | ASTM D257 |
Covestro Apec® DP9-9333 High-Heat Polycarbonate, General Purpose, UV-Stabilized
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
Covestro Makrolon® SF-800 Polycarbonate, Structural Foam
(discontinued **) Properties based on foam density of 0.90 g/cc.Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially.. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | Average value: 1.00e+16 ohm-cm Grade Count:7 |
Overview of materials for Polypropylene with 20% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini.. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | |
Idemitsu Kosan Xarec® WA 212 SPS, 30% Glass Filled Crystalline Polymer, Glass Filled, Impact Modified. Used in Automotive and Industrial applications. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | |
Idemitsu Kosan Xarec® WA 212LG SPS, 30% Glass Filled |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | |
Idemitsu Kosan Xarec® WA 214 SPS, 40% Glass Filled |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
Borealis Borcell™ HE1102 High Density Polyethylene Compound for Gas Injection of Cellular Communication Cable Insulation Borcell HE1102 is a high density polyethylene. A nucleating agent is incorporated for a uniform and closed cell structure. The components in the formulation are selected to give the lowest possibl.. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
Borealis Borstar® HE6067 Black Bimodal HD Polyethylene Compound for Jacketing of Communication and Power Cables Borstar HE6067 is a black, bimodal, co-polymer high density polyethylene (HDPE) compound produced according to the bimodal Borstar process. It is characterized by its balanced properties important .. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
Toyobo TS301 PPS, 30% Glass Fiber Reinforced Key Feature: Excellent impact resistance, high flowHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology developed by Toyobo.. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
Toyobo Vylopet® EMC330K Glass Reinforced Polyester, Easy Molding Grade HB UL-94 classApplications: General and high rigidity componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strength and tracking resistance, c.. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
Toyobo Vylopet® EMC430 PET/PBT Blend Key Feature: HB UL-94 ClassApplications: general and high rigidity componentsPET/PBT blends suggested for glossy surfaces. General features of Vylopet® include heat resistance, good mechanical pro.. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | IEC 112 |
Covestro Bayblend® T 45 Polycarbonate/ABS Blend High impact and notched impact strength, little risk of brittle fracture, high dimensional accuracy, good platable.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was sep.. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | |
Ceradyne Ceralloy® 147-A Hot Pressed Silicon Nitride (Si3N4) Ceralloy® 147 Reaction Bonded Silicon Nitride (RBSN) is a high purity grade of silicon nitride. RBSN has excellent thermal shock resistance and outstanding compatibility with non-ferrous molten met.. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
PolyOne Lubri-Tech™ AT-000/15T-2S Copolymer Acetal - 15% PTFE, 2% Silicone Lubricated
(discontinued **) Data provided by PolyOne. |
|||
Electrical Resistivity | 1.00e+16 - 1.00e+17 ohm-cm | 1.00e+16 - 1.00e+17 ohm-cm | Average value: 7.75e+16 ohm-cm Grade Count:4 |
Overview of materials for Acrylic, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values o.. |