Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00110 ohm-cm | 0.00110 ohm-cm | |
UCAR Carbon UCAR® ATJ Isostatic Molded Graphite Isostatically molded ATJ has been an industry standard for many years. It is a fine grain, high strength material which can be machined to precise tolerances and a fine surface finish. Grade ATJ has.. |