Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0001082 ohm-cm | 0.0001082 ohm-cm | |
Carpenter 20Cb-3® Stainless Steel Data provided by Carpenter Technology Corporation.20Cb-3® is an austenitic stainless steel possessing excellent resistance to hot sulfuric acid and many other aggressive environments which would re.. |
|||
Electrical Resistivity | 0.0001082 ohm-cm | 0.0001082 ohm-cm | |
Carpenter 20Cb-3® Stainless Steel, Bar, Annealed at 1750°F (955°C) then Water Quenched Data provided by Carpenter Technology Corporation.20Cb-3® is an austenitic stainless steel possessing excellent resistance to hot sulfuric acid and many other aggressive environments which would re.. |
|||
Electrical Resistivity | 0.0001082 ohm-cm | 0.0001082 ohm-cm | |
Carpenter 20Cb-3® Stainless Steel, Strip, Annealed at 1750°F (955°C) then Water Quenched Data provided by Carpenter Technology Corporation.20Cb-3® is an austenitic stainless steel possessing excellent resistance to hot sulfuric acid and many other aggressive environments which would re.. |
|||
Electrical Resistivity | 0.0001082 ohm-cm | 0.0001082 ohm-cm | |
Carpenter 20-Mo6® Stainless Steel, Plate Data provided by Carpenter Technology Corporation.This is an austenitic stainless steel which is resistant to corrosion in hot chloride environments with low pH. It has good resistance to pitting, .. |
|||
Electrical Resistivity | 0.0001082 ohm-cm | 0.0001082 ohm-cm | |
Carpenter 20-Mo6® Stainless Steel, Strip Data provided by Carpenter Technology Corporation.This is an austenitic stainless steel which is resistant to corrosion in hot chloride environments with low pH. It has good resistance to pitting, .. |
|||
Electrical Resistivity | 0.0001082 ohm-cm | 0.0001082 ohm-cm | |
Carpenter 20-Mo6® Stainless Steel, Tensile Properties at 93°C Data provided by Carpenter Technology Corporation.This is an austenitic stainless steel which is resistant to corrosion in hot chloride environments with low pH. It has good resistance to pitting, .. |