Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.000105 ohm-cm @Temperature 200 °C |
0.000105 ohm-cm @Temperature 392 °F |
|
Haynes 188 alloy, 0% cold reduction, 3.2 mm thick sheet Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Electrical Resistivity | 0.000105 ohm-cm @Temperature 200 °C |
0.000105 ohm-cm @Temperature 392 °F |
|
Haynes 188 alloy, 10% cold reduction, 3.2 mm thick sheet, 1065°C for 5 minutes Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Electrical Resistivity | 0.000105 ohm-cm @Temperature 200 °C |
0.000105 ohm-cm @Temperature 392 °F |
|
Haynes 188 alloy, 10% cold reduction, 3.2 mm thick sheet, 1175°C for 5 minutes Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Electrical Resistivity | 0.000105 ohm-cm @Temperature 200 °C |
0.000105 ohm-cm @Temperature 392 °F |
|
Haynes 188 alloy, 20% cold reduction, 3.2 mm thick sheet Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Electrical Resistivity | 0.000105 ohm-cm @Temperature 200 °C |
0.000105 ohm-cm @Temperature 392 °F |
|
Haynes 188 alloy, 20% cold reduction, 3.2 mm thick sheet, 1065°C for 5 minutes Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Electrical Resistivity | 0.000105 ohm-cm @Temperature 200 °C |
0.000105 ohm-cm @Temperature 392 °F |
|
Haynes 188 alloy, 20% cold reduction, 3.2 mm thick sheet, 1120°C for 5 minutes Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Electrical Resistivity | 0.000105 ohm-cm @Temperature 200 °C |
0.000105 ohm-cm @Temperature 392 °F |
|
Haynes 188 alloy, 20% cold reduction, 3.2 mm thick sheet, 1175°C for 5 minutes Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Electrical Resistivity | 0.000105 ohm-cm @Temperature 200 °C |
0.000105 ohm-cm @Temperature 392 °F |
|
Haynes 188 alloy, 30% cold reduction, 3.2 mm thick sheet Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Electrical Resistivity | 0.000105 ohm-cm @Temperature 200 °C |
0.000105 ohm-cm @Temperature 392 °F |
|
Haynes 188 alloy, 30% cold reduction, 3.2 mm thick sheet, 1065°C for 5 minutes Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Electrical Resistivity | 0.000105 ohm-cm @Temperature 200 °C |
0.000105 ohm-cm @Temperature 392 °F |
|
Haynes 188 alloy, 30% cold reduction, 3.2 mm thick sheet, 1120°C for 5 minutes Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Electrical Resistivity | 0.000105 ohm-cm @Temperature 200 °C |
0.000105 ohm-cm @Temperature 392 °F |
|
Haynes 188 alloy, 30% cold reduction, 3.2 mm thick sheet, 1175°C for 5 minutes Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Electrical Resistivity | 0.000105 ohm-cm @Temperature 200 °C |
0.000105 ohm-cm @Temperature 392 °F |
|
Haynes 188 alloy, 40% cold reduction, 3.2 mm thick sheet Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Electrical Resistivity | 0.000105 ohm-cm @Temperature 200 °C |
0.000105 ohm-cm @Temperature 392 °F |
|
Haynes 188 alloy, 40% cold reduction, 3.2 mm thick sheet, 1065°C for 5 minutes Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Electrical Resistivity | 0.000105 ohm-cm @Temperature 200 °C |
0.000105 ohm-cm @Temperature 392 °F |
|
Haynes 188 alloy, 40% cold reduction, 3.2 mm thick sheet, 1120°C for 5 minutes Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Electrical Resistivity | 0.000105 ohm-cm @Temperature 200 °C |
0.000105 ohm-cm @Temperature 392 °F |
|
Haynes 188 alloy, 40% cold reduction, 3.2 mm thick sheet, 1175°C for 5 minutes Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Electrical Resistivity | 0.000105 ohm-cm @Temperature 200 °C |
0.000105 ohm-cm @Temperature 392 °F |
|
Haynes 188 alloy, hot rolled and 1175°C solution annealed plate Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Electrical Resistivity | 0.000105 ohm-cm @Temperature 200 °C |
0.000105 ohm-cm @Temperature 392 °F |
|
Haynes 188 alloy, plate at RT after 0 hours at 870°C (1600°F) Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Electrical Resistivity | 0.000105 ohm-cm @Temperature 200 °C |
0.000105 ohm-cm @Temperature 392 °F |
|
Haynes 188 alloy, plate at RT after 1000 hours at 870°C (1600°F) Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Electrical Resistivity | 0.000105 ohm-cm @Temperature 200 °C |
0.000105 ohm-cm @Temperature 392 °F |
|
Haynes 188 alloy, plate at RT after 16000 hours at 870°C (1600°F) Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Electrical Resistivity | 0.000105 ohm-cm @Temperature 200 °C |
0.000105 ohm-cm @Temperature 392 °F |
|
Haynes 188 alloy, plate at RT after 4000 hours at 870°C (1600°F) Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Electrical Resistivity | 0.000105 ohm-cm @Temperature 200 °C |
0.000105 ohm-cm @Temperature 392 °F |
|
Haynes 188 alloy, plate at RT after 8000 hours at 650°C (1200°F) Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Electrical Resistivity | 0.000105 ohm-cm @Temperature 200 °C |
0.000105 ohm-cm @Temperature 392 °F |
|
Haynes 188 alloy, plate at RT after 8000 hours at 870°C (1600°F) Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Electrical Resistivity | 0.000105 ohm-cm @Temperature 200 °C |
0.000105 ohm-cm @Temperature 392 °F |
|
Haynes 188 alloy, 10% cold reduction, 3.2 mm thick sheet Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Electrical Resistivity | 0.000105 ohm-cm @Temperature 200 °C |
0.000105 ohm-cm @Temperature 392 °F |
|
Haynes 188 alloy, 10% cold reduction, 3.2 mm thick sheet, 1120°C for 5 minutes Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Electrical Resistivity | 0.000105 ohm-cm @Temperature 200 °C |
0.000105 ohm-cm @Temperature 392 °F |
|
Haynes 188 alloy, cold rolled and 1175°C solution annealed sheet Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Electrical Resistivity | 0.000105 ohm-cm @Temperature 200 °C |
0.000105 ohm-cm @Temperature 392 °F |
|
Haynes 188 alloy, plate at RT after 8000 hours at 760°C (1400°F) Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Electrical Resistivity | 0.000105 - 0.000110 ohm-cm | 0.000105 - 0.000110 ohm-cm | |
AMT AM-Lite® Die Casting Magnesium Alloy AM-lite is a high surface finish die casting alloy suitable for applications that currently utilize zinc, aluminum or magnesium (alloy AZ91D) die castings, or plastic injection moldings. AM-lite has.. |