Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000870 ohm-cm | 0.0000870 ohm-cm | RT |
Outokumpu 4828 High Temperature Austenitic Stainless Steel Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and .. |
|||
Electrical Resistivity | 0.0000870 ohm-cm | 0.0000870 ohm-cm | RT |
Outokumpu 4833 High Temperature Austenitic Stainless Steel Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and .. |