Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000850 ohm-cm @Temperature 100 °C |
0.0000850 ohm-cm @Temperature 212 °F |
|
Outokumpu 2205 Duplex Stainless Steel Duplex stainless combining high mechanical strength with good corrosion resistance.Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical t.. |
|||
Electrical Resistivity | 0.0000850 ohm-cm | 0.0000850 ohm-cm | RT |
Outokumpu 254 SMO® High Performance Austenitic Stainless Steel Applications: Process equipment in chemical industryBleaching equipment in the pulp and paper industryFlue-gas cleaningDesalinationSeawater handlingHeat exchangersAvailable in hot rolled plate (Quar.. |
|||
Electrical Resistivity | 0.0000850 ohm-cm | 0.0000850 ohm-cm | RT |
Outokumpu 4429 Cr-Ni-Mo Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), cold rolled strip/sheet and rod forms. |
|||
Electrical Resistivity | 0.0000850 ohm-cm | 0.0000850 ohm-cm | RT |
Outokumpu 4438 High Performance Austenitic Stainless Steel Very good corrosion resistance, weldable, and resistant to sensitization.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar,.. |
|||
Electrical Resistivity | 0.0000850 ohm-cm | 0.0000850 ohm-cm | RT |
Outokumpu 4439 Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), and cold rolled strip/sheet forms. |
|||
Electrical Resistivity | 0.0000850 ohm-cm @Temperature 100 °C |
0.0000850 ohm-cm @Temperature 212 °F |
|
Outokumpu SAF 2304® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |
|||
Electrical Resistivity | 0.0000850 ohm-cm @Temperature 100 °C |
0.0000850 ohm-cm @Temperature 212 °F |
|
Outokumpu SAF 2507® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |
|||
Electrical Resistivity | 0.0000850 ohm-cm @Temperature 20.0 °C |
0.0000850 ohm-cm @Temperature 68.0 °F |
|
Industeel URANUS® 52N+ 25 Cr Super Duplex Stainless Steel with PREN = 40 Description: URANUS® 52N+ (UR 52N+) is a super duplex stainless steel with 25% Cr and a PREN value higher than 40. The minimum guaranteed yield strength is 550 MPa which allows the designer to re.. |
|||
Electrical Resistivity | 0.0000850 ohm-cm @Temperature 20.0 °C |
0.0000850 ohm-cm @Temperature 68.0 °F |
|
Industeel URANUS® 47N+ 25 Cr Super Duplex Stainless Steel with PREN = 40 Description: CLI - SAF 2507® is a 25.07 super duplex stainless steel with 25% Cr and a PREN value higher than 40. The minimum guaranteed yield strength is 550 MPa which allows the designer to red.. |
|||
Electrical Resistivity | 0.0000850 ohm-cm @Temperature 100 °C |
0.0000850 ohm-cm @Temperature 212 °F |
|
Outokumpu LDX 2101® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |