Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000720 ohm-cm @Temperature 23.0 °C |
0.0000720 ohm-cm @Temperature 73.4 °F |
|
Crucible Steel 321 Chromium-Nickel Steel Crucible 321 is a non-hardenable, low carbon austenitic chromium-nickel steel which is particularly adaptable for parts fabricated by welding without postweld annealing for use at temperatures betwe.. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
AK Steel 304 Austenitic Stainless steel AK Steel 304 is a variation of the basic 18-8 grade, Type 302. Lower carbon, in Type 304, minimizes chromium carbide precipitation due to welding and its susceptibility to intergranular corrosion. .. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
AK Steel 305 Austenitic Stainless steel AK Steel 305 can be spun and deep drawn more easily due to an increased nickel content that decreases work hardening. It is non-magnetic and cannot be hardened by heat treatment. Typical uses incl.. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
AK Steel 321 Austenitic Stainless steel AK Steel 321 is a stabilized austenitic stainless steel similar to Type 304 but with a titanium addition. This titanium addition reduces or prevents carbide precipitation during welding and in 427 .. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, 20% Cold Rolled (UNS S30200) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, 30% Cold Rolled (UNS S30200) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, Annealed (UNS S30200) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, 10% Cold Rolled (UNS S30400) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, 50% Cold Rolled (UNS S30400) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, 0% Cold Rolled (UNS S30403) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, 10% Cold Rolled (UNS S30403) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, 50% Cold Rolled (UNS S30403) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 305, 40% Cold Rolled (UNS S30500) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 305, 50% Cold Rolled (UNS S30500) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 305, 60% Cold Rolled (UNS S30500) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 305, Annealed (UNS S30500) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 303, Annealed (UNS S30300) Allegheny Ludlum's 303 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties.. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
Carlson 303 Austenitic Stainless Steel Carlson 303 is an austenitic free-machining stainless steel. The standard 18-8 stainless steels are more difficult to turn, mill and drill which restricts their use when considerable machining is r.. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, 10% Cold Rolled (UNS S30200) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, 50% Cold Rolled (UNS S30200) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, 60% Cold Rolled (UNS S30200) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, 0% Cold Rolled (UNS S30400) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, 30% Cold Rolled (UNS S30400) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Type 301, 1/2 Hard (UNS S30100) Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho.. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Type 301, 1/4 Hard (UNS S30100) Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho.. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Type 301, annealed (UNS S30100) Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho.. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, 60% Cold Rolled (UNS S30400) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, 20% Cold Rolled (UNS S30403) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 305, 20% Cold Rolled (UNS S30500) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Electrical Resistivity | 0.0000720 ohm-cm | 0.0000720 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Type 321 (UNS S32100) AL 321 is a stabilized stainless steel which offers excellent resistance to intergranular corrosion following exposure to temperatures in the chromium carbide precipitation range from 800° to 1500°.. |